Share
Page 1 of 3 123 LastLast
Results 1 to 20 of 42

Thread: Sneak peak at 2016 models.

  1. #1

    Default Sneak peak at 2016 models.

    We are slowly integrating some new improved models into the pipeline for mid year and into the late fall. I know that a lot of people are going to want to know when, where, how, etc. But that's not the exact point of this thread. Know how car magazines try to get glimpses of long rumored products...pictures of the mules or ready for production pre-release fun drives? That's this thread. So...we'll give out the information details more when we have things fully in stock. We will have a few of these models being released and integrated as we go. Already we have a couple.

    But let's talk about what is going on a bit behind the scenes here... A good bit of our line as you know is digital. And it's proven to be reliable and serviceable with the modular component design where items or commonalized (is that a word?) to improve long term repair and service.

    A few of our products that you know are digital:
    PowerTIG 210EXT
    PowerTIG 255EXT
    PowerTIG 325EXT
    Power iTIG 200T
    PowerARC 280STH

    A few of our products that you may not know are already digital:
    PowerMTS 250S
    PowerMTS 200
    Power iMIG 200
    Power iMIG 205

    And we have a few more that will be digitalized(or is it digitized the more accepted term?) this year and released as the 2016 models...some already here in limited quantities for select customers.

    A few of you are wondering about what we define as DIGITAL. That's a good question and definitely a valid one.

    A lot of people see electronics and digital displays and think the unit is digital.
    No, it's not necessarily so.

    Some people see knobs and automatically think it's analog.
    No, it's not so.

    I am probably not qualified enough to point out the fine points in digital versus analog. I'll leave that to those that are. However, I constantly hear, "I'd rather have analog, they are simpler and I can work on it or its less trouble." Admittedly I thought the same thing when we first started considering digital production of some TIGs. But in reality, the digital versions have been far less complicated, weigh less, and have fewer parts and discreet circuits. In some cases, a single board design which makes repair and service quite easy, especially for customers a long way from our service facility who might be able to repair themselves. The biggest advantage is that it makes upgrading programming or refitting welders a possibility (as you will see in the video clip below) without having to completely rewire and retrofit components and part so that the newest versions will gee haw ( get along) with the older parts.

    As we seek to define digital production for us and our goals for 2016 and onward, we are simply designating the unit as digital if the major processes of the unit are digitally controlled with a microcontroller (processor). The units may still feature control knobs which are either analog pots or digital encoders. For our new small MIG line (the 200 and 205), they are digitally controlled with analog potentiometers. But the MTS units have knobs that are digital encoders. Anyway google digital encoder if you don't know what it is. Both have been reliable and have improved our products greatly, not only in reliability, but also in the quality feel they have and the features we can offer.

    As we promised our customers when we brought out the new digital line, the old line units weren't going anywhere, but if anything they'd be improved. And that's what we've done as we've begun to digitalize them. Yep. The new 250EX will be running a microcontroller and as you will see in the video I've put together with a couple short sneak peak clips from Duncan, it's the same 250EX, but it's not... it's better, simpler and well a whole lot neater inside. Still have the basic look and feel of the 250EX, but with a couple of minor differences. One we've done away with the rocker switches and replaced them with touch pads. This isn't wholly bad as now you can actually see from a distance what setting you've selected as it will be lit up.


    This is a sneak peak at the NEW 250EX.

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Very interesting. I know there are a lot of people that prefer the rows of knobs vs. having to step through menus. Looks like this is the best of both worlds. Thanks for the peek.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    Sweet! I prefer the knobs over the menus, which is why I never stepped up to the 255.
    Gerald

    Millermatic 251
    Spectrum 300 Plasma
    Everlast PowerTig 250EX
    Everlast PowerCool W300
    Harris / Victor OA
    Craftsman 13 Speed Drill Press
    ProTools Air/Hydraulic Bender
    48" Brake, 72" Brake, 52" Stomp Shear
    Mitler Bros. 36" High Throat Bead Roller
    Compressor, Notchers, Grinders, etc.

  4. Default

    I prefer the knobs my self. I like that I can know at a glance what the settings are. I am sure digital simplifies things for Everlast. I do not know if I am completely sold on digital though. I guess if it alows Everlast to diagnose it over the phone and send out a board it would be worth going to it. The concern I have with digital is that problems are more apt to come and go. I am concerned about this throw away society we live in. The younger people think that if they get 3-4 years out of an electronic tool that that is aceptabe. I grew up with the perseption that if you buy a good product you will have it for the rest of your life. I have a few welders that are almost as old as I am and they still work fine. That said, those old welders do not have many of the new features and are heavy and large so wether I like it or not digital is here to stay. One concern I do have is that with models changing drastically from year to year is availability of parts and the knowledge to repair a machine that is only made for a year or two. So for that reason I would want the latest version of the welder. I will be ordering one soon myself so I do appreciate the sneak peak.
    Miller 302 gas drive
    millermatic 200 mig
    miller spoolmatic 3 spool gun with 100ft ext.
    2014 Everlast PP60S plasma
    thermal arc 250 GTS inverter
    2016 Everlast 250EX
    miller tig cooler
    2015 Everlast MTS250S
    Miller 30A spool Gun
    Miller xtreme 12VS wire feeder
    Linde CM 85 shape cutter

  5. #5

    Default

    Gary,

    The digital reduces the amount of circuitry. That is a good thing on any level. The digital will either work or it won't and we don't see too many issues with it. The issue with analog to an extent is that is the exact issue that we have at times that you've assigned to digital. As far as changing regularly, the 250EX has remained relatively unchanged for the last couple years. And definitely the 200DV has as well. But I doubt we'll see much more change now.

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by performance View Post
    But I doubt we'll see much more change now.
    People have been saying that for a long time. The only constant is change.

    There is room for both old and new, expensive lifetime products as well as cheaper limited life things. Each has it's place. Everyone talks about obsolescence, but we still dig holes with shovels.
    Long arc, short arc, heliarc and in-the-dark!

  7. #7

    Default

    I mean, as our 250EX has reached its final major regeneration for now and hope it will continue to be a great seller. We've reached a point of getting the units where we've been aiming for the last 5 years...but you are right...We are thinking about a few extra things to tweak them here or there and who knows enter the 251EX era?

  8. #8

    Default

    New i TIG 200 in the vein of the new 250EX. Units after July will be renamed Power iTIG 201 so...
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	new_i-TIG200_side_view.jpg 
Views:	1293 
Size:	135.0 KB 
ID:	13013  

  9. Default

    will the 250 ex be dual voltage?

  10. #10

    Default

    Not that I am aware of. I am waiting for final spec sheet on the unit. Duncan is over there now.

  11. Default

    cool Mark I will give you a call on Mon gonna send in my 210ext but buy the new mts251 i and maybe a couple more welders this next month. I ran my 140 power arc for 10 hour a day running 7018 for a week and it didnt let me down on 220 on 110 its kind of a eratic arc but I am stoked after it got me through this structural job. I am going all green this year.

  12. Default

    Wow!

    That Power iTIG 201 unit is brilliant.

    I mean, it's a full-featured AC/DC unit in a compact form, at $699.

    Wow!

    Peace to you all,
    C. Livingstone
    Last edited by christian; 08-03-2015 at 01:49 PM.

  13. #13

    Default

    No, it's DC only.

  14. Default

    OH, gee,

    My bad!

    I saw the Pulse and what looks like Frequency control and figured it was AC too.

    Also though, in the Products section of the Everlast website, even though there's no picture, it does list the proposed iTIG 201 unit as an AC/DC one.

    Peace to you all,
    C. Livingstone
    Last edited by christian; 08-03-2015 at 06:03 PM.

  15. #15
    Join Date
    Oct 2013
    Location
    Glendale Arizona
    Posts
    26

    Default

    Quote Originally Posted by christian View Post
    OH, gee,

    My bad!

    I saw the Pulse and what looks like Frequency control and figured it was AC too.

    Also though, in the Products section of the Everlast website, even though there's no picture, it does list the proposed iTIG 201 unit as an AC/DC one.

    Peace to you all,
    C. Livingstone
    I saw a post on the iTIG 200 on another site about this being competitive with the AHP. Took a look over here and it doe say AC/DC and was just waiting for more info and a release date. Oh well, back to yellow.

  16. Default

    Yeah,

    It seems like there might still be some ambiguity. I mean, if you look at the photo, there is a knob for "Balance", i.e., AC Balance.

    So, maybe Mark would be willing to double check for us.

    Peace to you all,
    C. Livingstone

  17. #17
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Power iTIGs are DC only machines much like the Miller Maxstar line. That is not likely to change. The frequency and cycle controls you see are for the pulser.
    Long arc, short arc, heliarc and in-the-dark!

  18. Default

    OK,

    DC it is.

    Peace to you all,
    C. Livingstone

  19. #19

    Default

    Do any of the 2016 Tig or Mig welders have 'fan on demand' functionality?
    imig 200
    PowerTig 210 EXT

  20. #20

    Default

    Quote Originally Posted by johnnymg View Post
    Do any of the 2016 Tig or Mig welders have 'fan on demand' functionality?
    What and ruin our duty cycle like everyone else has? No. There are no plans for any part time cooling.

Similar Threads

  1. How about some 220v -440v single phase models
    By TheGary in forum Pre-sales, Sales and Shipping questions
    Replies: 0
    Last Post: 01-16-2016, 07:16 PM
  2. new models in the pipeline
    By TheGary in forum Everlast Announcements, Contests and Promotions
    Replies: 1
    Last Post: 05-18-2015, 05:47 PM
  3. Are the new 2013 models out yet?
    By mrflashlite in forum Pre-sales, Sales and Shipping questions
    Replies: 52
    Last Post: 03-06-2013, 06:25 PM
  4. October special on the NEW units and models.
    By admin in forum Everlast Announcements, Contests and Promotions
    Replies: 2
    Last Post: 10-25-2008, 12:14 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •