    There is no way you can weld a soda can with this welder the arc to to unstable at the low amps or is a problem with the machine

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,662

    Default

    Have you tried a new bottle of argon? As you can see from this thread, that fixed Steve's problem.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3
    Join Date
    Jul 2015
    Location
    san leandro CA
    Posts
    17

    Default

    No i will try it see what happens thanks

  4. #4

    Default

    some people don't/won't/can't assimilate the info at hand.
    others TROLL
    ON my 250EX, problems have been operator error induced RTM (then reread)
    Last edited by rick9345; 08-10-2015 at 01:10 AM.

  5. #5
    Join Date
    Jul 2015
    Location
    san leandro CA
    Posts
    17

    Default

    I have read the RTM over and over i started welding at night but not last night but this is my first CHINESE WELDER . Operator error can not cause the arc to wonder and flutter and not start then blast like a blow torch then let off the pedal then the arc is barely there and its only on AC don't matter what the amps are the ARC SUCKS.

  6. #6

    Default

    Quote Originally Posted by slzboy View Post
    I have read the RTM over and over i started welding at night but not last night but this is my first CHINESE WELDER . Operator error can not cause the arc to wonder and flutter and not start then blast like a blow torch then let off the pedal then the arc is barely there and its only on AC don't matter what the amps are the ARC SUCKS.
    EDIT: Just noticed you had a separate thread already.

    Maybe start a new thread and list the settings and materials, etc, like the OP. This thread it wandering and he clearly said it was bad argon (sometime when tanks get low I notice this even on what was a good tank).

    Also, are you sure the other welders you have used have no Chinese parts or labor in them?
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Hate it when I get a call that starts out...
    By millerized in forum Other Custom Fabrications
    Replies: 4
    Last Post: 01-04-2015, 09:28 PM
  2. New 2015 PowerTIG 255EXT
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 34
    Last Post: 10-19-2014, 12:42 PM
  3. HF starts quit working - PowerTIG 200DX
    By Timebandit in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 09-04-2014, 02:04 PM
  4. Arc Starts
    By ArcRay in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 09-16-2013, 04:54 PM
  5. New issue with high amp arc starts on 160STH
    By youngnstudly in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 01-29-2013, 04:45 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •