    Quote Originally Posted by everlastsupport View Post
    I would call into tech support. Are the amps wide open when you try to use it (blowing holes in 1/8" metal plate)? Still on an older bottle of Argon?
    No its not wide open, it seems like what ever I change the start amp setting to it will use the entire time. Not sure how old the Argon is, how would the display readout be effected by gas quality?

  2. #2

    Default

    I was wondering if moisture was in the argon, that will make some amp issues and bad looking welds. So you are saying the up and down slope seem to not be working?
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Foot Control
    By kepp in forum Everlast Plasma Cutters (PAC)
    Replies: 12
    Last Post: 08-23-2012, 11:34 PM
  2. finger control
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 04-06-2012, 02:05 AM
  3. CNC control port
    By robsthomson in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 05-26-2011, 03:43 AM
  4. hand control
    By hammerbait in forum General Welder Questions
    Replies: 18
    Last Post: 02-27-2011, 10:11 AM
  5. new amp control
    By Rodsmachineshop in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 04-12-2010, 11:27 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •