I have a power-pro 256 purchased on 10/24/12. I have not had any issues with this machine until yesterday. Somehow the amp control knob does not change the amperage. Things I have noticed, the amp control works on cut setting. In the tig/stick setting the display shows the beginning amp control setting knob, Tig it will show 4-193 using the beginning amp knob, stick it will show 16-193 beginning amp knob. Things I have tried unplugging the foot peddle, I have tried reseating the connector and making sure it was tight, I tried using the torch switch. And yes I have made sure that I have the t2/t4 rocker set correctly. Any other things I could try?