    I have th power pro 256 and I went and turned it on like I always do and after about 30 seconds I heard a loud pop from inside the unit and it shut down and popped the circuit breaker. I wasnt welding or cutting with it yet and it had no load when this happened. Any ideas or thoughts out there on what may have happened it sounded to loud to just be a fuse but maybe a capacitor or something went bad it is still under warranty I just don't know what I need to do now for it. Maybe if any of the admin or representatives can send me a pm on what I should do now? Thanks

  2. #2

    Default

    I am going to take a wild ### guess and say it is a large wire wound resistor,,,,very similar to the ballast resistor you would have mounted on the fire wall of older cars...when they blow that makes one hell of noise..BANG...
    Some of those lies people tell about me, are true

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    You could be right about a cap, but since you're asking, I'm guessing a blown IGBT module. Whatever you let the smoke out of, you should call support as your next step.

    Long arc, short arc, heliarc and in-the-dark!

  4. #4

    Default

    Probably on the plasma side, which are not modules.

    Whatever the case though, call tech support at 207 right away. No need to try to check anything since this sounds catastrophic to the machine. I have found a wire under the cover or something before that rubbed or touched and made a sound but this is probably something else.

Similar Threads

  1. 200DX, what am I doing wrong?
    By rappy'97 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 09-08-2015, 11:59 AM
  2. What am I doing wrong???
    By Toby in forum TIG Welding (GTAW/GTAW-P)
    Replies: 36
    Last Post: 04-09-2013, 12:54 AM
  3. 210ext what am i doing wrong
    By pig75 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 25
    Last Post: 02-16-2013, 03:47 PM
  4. wrong helmet sent
    By bubbas55 in forum Pre-sales, Sales and Shipping questions
    Replies: 1
    Last Post: 12-01-2012, 08:21 PM
  5. Wrong pedal
    By daniel_l2 in forum Pre-sales, Sales and Shipping questions
    Replies: 11
    Last Post: 06-26-2012, 10:26 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •