  1. Default

    Trying to teach myself how to tig. Mainly steel what to you think of the powerarc 280

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    If you just want to do steel, you can start off with your PA300. You will learn a lot and will know more about what you want in a TIG machine. Everlast has some videos showing a TIG setup on the PA300 on their YouTube channel.
    Long arc, short arc, heliarc and in-the-dark!

  3. Default

    I have done some tig with the powerarc 140. Lift start tig

  4. Default

    I am looking to have more control and options

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    I would look at an AC/DC machine if you want to get into TIG beyond just a basic setup.
    Long arc, short arc, heliarc and in-the-dark!

  6. Default

    if you are not going to be into tig welding aluminum . I would not get the ac dc machine. They are much pricier than you need. Any of Everlasts machines that has HF start will work fine. You will in liklyhood not ever weld on any ferrous metal at anything over 200 amps. If you want a do anything machine that can weld copper or alum. get the ac dc machine 250 amp.
    Miller 302 gas drive
    millermatic 200 mig
    miller spoolmatic 3 spool gun with 100ft ext.
    2014 Everlast PP60S plasma
    thermal arc 250 GTS inverter
    2016 Everlast 250EX
    miller tig cooler
    2015 Everlast MTS250S
    Miller 30A spool Gun
    Miller xtreme 12VS wire feeder
    Linde CM 85 shape cutter

  7. Default

    What about the powerarc 280. Is that a good tig welder ?

Similar Threads

  1. Advice on new 255ext set up
    By Dedvetpath in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 01-01-2016, 02:32 PM
  2. Need advice. Striking an Arc. PowerArc200
    By Kansan in forum Stick Welding (SMAW)
    Replies: 8
    Last Post: 03-26-2015, 11:43 PM
  3. Some advice for the beginner
    By Beginner in forum TIG Welding (GTAW/GTAW-P)
    Replies: 13
    Last Post: 09-05-2014, 04:47 AM
  4. Possible project ... need advice
    By Oleg in forum Personal Projects (no welder required)
    Replies: 23
    Last Post: 02-16-2012, 07:15 AM
  5. New Meber Intro and Looking For Advice
    By metallurgist in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 07-06-2011, 04:22 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •