Thread: Advice on a tig welder

  1. Default Advice on a tig welder

    Started off with the power arc300 and I really do like it then I bought the imig 205 and that welder is fantastic now I am looking to buy a tig unit can anybody give me a suggestion on which one to buy thank you very much

  2. #2

    Default

    Tell us what you will be doing with it.

  3. Default

    Trying to teach myself how to tig. Mainly steel what to you think of the powerarc 280

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    If you just want to do steel, you can start off with your PA300. You will learn a lot and will know more about what you want in a TIG machine. Everlast has some videos showing a TIG setup on the PA300 on their YouTube channel.
    Long arc, short arc, heliarc and in-the-dark!

  5. Default

    I have done some tig with the powerarc 140. Lift start tig

  6. Default

    I am looking to have more control and options

  7. #7
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    I would look at an AC/DC machine if you want to get into TIG beyond just a basic setup.
    Long arc, short arc, heliarc and in-the-dark!

  8. Default

    if you are not going to be into tig welding aluminum . I would not get the ac dc machine. They are much pricier than you need. Any of Everlasts machines that has HF start will work fine. You will in liklyhood not ever weld on any ferrous metal at anything over 200 amps. If you want a do anything machine that can weld copper or alum. get the ac dc machine 250 amp.
    Miller 302 gas drive
    millermatic 200 mig
    miller spoolmatic 3 spool gun with 100ft ext.
    2014 Everlast PP60S plasma
    thermal arc 250 GTS inverter
    2016 Everlast 250EX
    miller tig cooler
    2015 Everlast MTS250S
    Miller 30A spool Gun
    Miller xtreme 12VS wire feeder
    Linde CM 85 shape cutter

  9. Default

    What about the powerarc 280. Is that a good tig welder ?

  10. Default

    Or is it more of a stick welder?

  11. #11

    Default

    No, it really is both. It has all the features you need for DC TIG but it also has all the features of stick you need. We wanted to create a machine that could do both and either function can stand on it's own. It's a very very nice unit that is well priced. I'd recommend it myself having used one.

  12. Default

    After reading about the power arc 280 it will do it all as far as tig and stick is concerned on all but aluminum. You could sell your power arc 300 because the 280 can do it all.
    Miller 302 gas drive
    millermatic 200 mig
    miller spoolmatic 3 spool gun with 100ft ext.
    2014 Everlast PP60S plasma
    thermal arc 250 GTS inverter
    2016 Everlast 250EX
    miller tig cooler
    2015 Everlast MTS250S
    Miller 30A spool Gun
    Miller xtreme 12VS wire feeder
    Linde CM 85 shape cutter

  13. Default

    Thanks for the input. This will be my forth everlast welder. Once I save up enough to buy it. I am very happy with my three units I have. Everlast welders are great

  14. #14

    Default

    I suggest buying one that can do anything like the 250EX. It costs more money but you'll be happy with it and you'll always have what you need.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  15. Default

    Quote Originally Posted by zoama View Post
    I suggest buying one that can do anything like the 250EX. It costs more money but you'll be happy with it and you'll always have what you need.
    There is something to be said for that. Seeing as you have already purchased 3 welders. A 250EX , your 205 mig and your power arc 300 you would be totally covered for about any kind of welding. Add a nice clean generator some time in the future and you could even go mobil if needed.

    One draw back to the 250EX is that to get its full potential you will need a tig cooler too. The main question you need to answer is, are you going to want/need to weld aluminum in the future. You can run an air cooled torch on it if you want to. I have been welding a long time and there are not that many times you will need to weld aluminum at over 175 amps. I had a propeller shop for 5 years and only hade an air cooled torch. A couple of times I had to preheat an aluminum part so I could weld it but had no problem doing it. The big advantage to me with the 250EX is that it has a very good duty cycle compared to its smaller brothers.
    Last edited by TheGary; 05-10-2015 at 12:51 AM.
    Miller 302 gas drive
    millermatic 200 mig
    miller spoolmatic 3 spool gun with 100ft ext.
    2014 Everlast PP60S plasma
    thermal arc 250 GTS inverter
    2016 Everlast 250EX
    miller tig cooler
    2015 Everlast MTS250S
    Miller 30A spool Gun
    Miller xtreme 12VS wire feeder
    Linde CM 85 shape cutter

  16. #16

    Default

    Also have the 250EX with the CK Flexlok Series 3 head air cooled. have welded 200 amps short duration, for anything under 180 amps AC/DC comfortable.

  17. #17

    Default

    If no aluminum you are going the right way. But I like what Zoama said, 250EX. Stick and AC/DC TIG and ton of power. You can get it all. Also, you can run a water line from a faucet and cool the torch. I have a really nice cooler I never use. So don't get stuck on the water cooler. Search for redneck water cooler here on the forum.

    Then you decide which of the other unit you sell off.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  18. Default

    Thanks for all the help I appreciate it

  19. #19
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    Quote Originally Posted by zoama View Post
    I suggest buying one that can do anything like the 250EX. It costs more money but you'll be happy with it and you'll always have what you need.
    I completely agree with this. Better to have it and not need it, than to not have it and need it! I jumped from the PowerArc 160 straight up to the 250EX and I am really glad I skipped the 225LX and the PowerTig 185. You can get by without the water cooler for awhile, but you will need to purchase an aircooled tig torch until you get a cooler.

    The A/C torch I bought is rated for 200amps AC (Off the top of my head, I wanna say it has a 20% duty cycle??? ) and 250amps DC, and I don't have a problem welding preheated 1/2" aluminum plate at 190 amps in VERY short runs. The torch spends more time disassembled cooling off by the fan than in my hand welding, but it does get the job done with no trouble otherwise (for now). I have to build a new welding cart before I can even begin to think about getting/making a water cooler, and it's simply not a priority with all of the other things I have going on. Someday though.....
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

Similar Threads

  1. Advice on new 255ext set up
    By Dedvetpath in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 01-01-2016, 02:32 PM
  2. Need advice. Striking an Arc. PowerArc200
    By Kansan in forum Stick Welding (SMAW)
    Replies: 8
    Last Post: 03-26-2015, 11:43 PM
  3. Some advice for the beginner
    By Beginner in forum TIG Welding (GTAW/GTAW-P)
    Replies: 13
    Last Post: 09-05-2014, 04:47 AM
  4. Possible project ... need advice
    By Oleg in forum Personal Projects (no welder required)
    Replies: 23
    Last Post: 02-16-2012, 07:15 AM
  5. New Meber Intro and Looking For Advice
    By metallurgist in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 07-06-2011, 04:22 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •