    I decided to make a cart for the 250 EX tig machine and my PP60. I tig welded the whole thing except for two small welds at the bottom that were done with the mig.
    Didn't really have a plan, I just cobbled it up out of what I had on hand. Everything had been rusting outside for a year other than the sheet metal. The frame is 1x1x1/8 hot roll, the sheet is 14ga hot roll.
    I tried making plug welds on the bottom shelf but they turned out looking like crap so I gave it another pass with the 7" 24 grit flap wheel. I just tacked the top every two inches, that worked much better for me.
    Click image for larger version. 

Name:	1.jpg 
Views:	711 
Size:	93.1 KB 
ID:	12966

    I wanted to mount the Motor Guard M60 dryer to the frame but it didn't come with a bracket, so I cut two pieces of 1/4x3 hot roll, welded them together and then plasma cut the bracket and cleaned it up on the belt sander.
    The dryer just sits in it and can be lifted out for service. The bottle brackets are made from the same 1/4x3 hot roll.

    Click image for larger version. 

Name:	2.jpg 
Views:	599 
Size:	57.1 KB 
ID:	12967Click image for larger version. 

Name:	3.jpg 
Views:	568 
Size:	83.1 KB 
ID:	12968

    My welds range from OK to crap but I'm practicing. Poor eyesight is my biggest problem, getting old sucks.

    Click image for larger version. 

Name:	4.jpg 
Views:	641 
Size:	98.8 KB 
ID:	12969Click image for larger version. 

Name:	5.jpg 
Views:	594 
Size:	110.4 KB 
ID:	12970

    I shot it with semi-flat black Rustoleum. The primer ran like water but it'll work.

    Click image for larger version. 

Name:	6.jpg 
Views:	596 
Size:	85.9 KB 
ID:	12971Click image for larger version. 

Name:	7.jpg 
Views:	605 
Size:	123.8 KB 
ID:	12972Click image for larger version. 

Name:	8.jpg 
Views:	765 
Size:	116.3 KB 
ID:	12973

    The caster brackets were cut from two pieces of 1x4 cold roll, then cut in half on the horizontal band saw to make them about 1/2" thick and threaded 1/2x13 for the 5" ball bearing total lock casters.
    I like casters on all four corners so I can move it in any direction. The cart doesn't go outside. The casters cost about $9 each and work great. http://www.ebay.com/itm/151428117977?_
    I put them on everything that needs to roll in my shop.

    Click image for larger version. 

Name:	9.jpg 
Views:	667 
Size:	112.2 KB 
ID:	12974Click image for larger version. 

Name:	10.jpg 
Views:	613 
Size:	104.8 KB 
ID:	12975

    I'm happy with it, it suits me.
    Last edited by zoama; 07-19-2015 at 10:19 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

Similar Threads

  1. Recent Project (250EX) - Welding Cart from Hell
    By Gandalf in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 08-30-2013, 04:42 AM
  2. 250EX-Aluminum welding cart
    By 5440 in forum Other Custom Fabrications
    Replies: 19
    Last Post: 03-25-2013, 10:18 AM
  3. Replies: 13
    Last Post: 03-25-2012, 05:28 PM
  4. First Welding Project - You guessed it... a welding cart
    By EmptyNester in forum Hobyist Projects
    Replies: 19
    Last Post: 10-12-2011, 03:30 PM
  5. Pa200/ PP60 welder cart
    By Scooter in forum Other Custom Fabrications
    Replies: 4
    Last Post: 05-13-2011, 07:15 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •