Share
Results 1 to 20 of 20

Thread: Welding Cart For 250EX And PP60 Plasma Cutter+ Boat Project

  1. #1

    Default Welding Cart For 250EX And PP60 Plasma Cutter+ Boat Project

    I decided to make a cart for the 250 EX tig machine and my PP60. I tig welded the whole thing except for two small welds at the bottom that were done with the mig.
    Didn't really have a plan, I just cobbled it up out of what I had on hand. Everything had been rusting outside for a year other than the sheet metal. The frame is 1x1x1/8 hot roll, the sheet is 14ga hot roll.
    I tried making plug welds on the bottom shelf but they turned out looking like crap so I gave it another pass with the 7" 24 grit flap wheel. I just tacked the top every two inches, that worked much better for me.
    Click image for larger version. 

Name:	1.jpg 
Views:	1664 
Size:	93.1 KB 
ID:	12966

    I wanted to mount the Motor Guard M60 dryer to the frame but it didn't come with a bracket, so I cut two pieces of 1/4x3 hot roll, welded them together and then plasma cut the bracket and cleaned it up on the belt sander.
    The dryer just sits in it and can be lifted out for service. The bottle brackets are made from the same 1/4x3 hot roll.

    Click image for larger version. 

Name:	2.jpg 
Views:	1502 
Size:	57.1 KB 
ID:	12967Click image for larger version. 

Name:	3.jpg 
Views:	1522 
Size:	83.1 KB 
ID:	12968

    My welds range from OK to crap but I'm practicing. Poor eyesight is my biggest problem, getting old sucks.

    Click image for larger version. 

Name:	4.jpg 
Views:	1605 
Size:	98.8 KB 
ID:	12969Click image for larger version. 

Name:	5.jpg 
Views:	1577 
Size:	110.4 KB 
ID:	12970

    I shot it with semi-flat black Rustoleum. The primer ran like water but it'll work.

    Click image for larger version. 

Name:	6.jpg 
Views:	1508 
Size:	85.9 KB 
ID:	12971Click image for larger version. 

Name:	7.jpg 
Views:	1554 
Size:	123.8 KB 
ID:	12972Click image for larger version. 

Name:	8.jpg 
Views:	1716 
Size:	116.3 KB 
ID:	12973

    The caster brackets were cut from two pieces of 1x4 cold roll, then cut in half on the horizontal band saw to make them about 1/2" thick and threaded 1/2x13 for the 5" ball bearing total lock casters.
    I like casters on all four corners so I can move it in any direction. The cart doesn't go outside. The casters cost about $9 each and work great. http://www.ebay.com/itm/151428117977?_
    I put them on everything that needs to roll in my shop.

    Click image for larger version. 

Name:	9.jpg 
Views:	1603 
Size:	112.2 KB 
ID:	12974Click image for larger version. 

Name:	10.jpg 
Views:	1509 
Size:	104.8 KB 
ID:	12975

    I'm happy with it, it suits me.
    Last edited by zoama; 07-19-2015 at 10:19 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Looks good, to me. I especially like your pieced together dryer bracket. I'd be lost without a cheater lens, in my helmet, these days.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    Quote Originally Posted by Rambozo View Post
    Looks good, to me. I especially like your pieced together dryer bracket. I'd be lost without a cheater lens, in my helmet, these days.
    Thanks, I use my bifocals but when I get in an odd position I lose focus and start guessing.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4
    Join Date
    Dec 2011
    Location
    RUSSIA.Sankt Peterburg
    Posts
    218

    Default

    Excellent cart , good job !!!
    Ruslan
    EVERLAST Power Tig 255 EXT
    EVERLAST PP256
    PC300
    EWM Pico 162
    MERKLE mobimig 180K
    SELCO Genesis 352 pme

  5. #5

    Default

    Quote Originally Posted by donor76 View Post
    Excellent cart , good job !!!
    Thank you.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. #6

    Default

    To the guys who have looked at my cart...

    What would you have done different ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. #7

    Default

    Can't see anything I would change. Heck if Donor76 says it is nice, can't get much better than that. Maybe a self or something to clutter up with consumables
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  8. #8

    Default

    A little 16v Lund boat project with my silly assistant trying to help. Click image for larger version. 

Name:	11.jpg 
Views:	1470 
Size:	143.8 KB 
ID:	13031Click image for larger version. 

Name:	12.jpg 
Views:	1449 
Size:	141.7 KB 
ID:	13032Click image for larger version. 

Name:	13.jpg 
Views:	1457 
Size:	145.6 KB 
ID:	13033
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  9. #9

    Default

    The 1975 boat had a tree fall on it, caving in the starboard side where the drivers console used to be. I've stripped the boat, straightened the side and replaced the gunnels with the latest dual mounting rail design.
    Now it's getting a 3/16" 5052 H32 floor along with new rod lockers on both sides, a rear bench for the new tiller steer, two seat pedestals, a live well and a short platform at the bow to mount a trolling motor.
    The only wood on the boat will be two new layers of 3/4" marine plywood in the transom.

    The new gunwale design (gunnel).
    Click image for larger version. 

Name:	14.jpg 
Views:	1391 
Size:	87.1 KB 
ID:	13034
    Last edited by zoama; 06-23-2015 at 02:21 AM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  10. #10
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Looking forward to your progress reports. Just had a boat come back yesterday and the gunwale is breaking loose from the transom and the hull. Looks like I will also have a project. I knew the transom was going to let go one of these days anyway. On our last fiberglass boat, I replaced the outboard transom plate from plywood to a sheet of polypropylene. That worked out very well, so I was planning on redoing this aluminum/plywood transom, with aluminum/polypropylene. I've never been a big fan of mixing wood and water.

    How are you going to form that gunwale extrusion? I might use something like that to replace the round tube I have now.
    Long arc, short arc, heliarc and in-the-dark!

  11. #11

    Default

    Quote Originally Posted by Rambozo View Post
    Looking forward to your progress reports. Just had a boat come back yesterday and the gunwale is breaking loose from the transom and the hull. Looks like I will also have a project. I knew the transom was going to let go one of these days anyway. On our last fiberglass boat, I replaced the outboard transom plate from plywood to a sheet of polypropylene. That worked out very well, so I was planning on redoing this aluminum/plywood transom, with aluminum/polypropylene. I've never been a big fan of mixing wood and water.

    How are you going to form that gunwale extrusion? I might use something like that to replace the round tube I have now.
    The new gunwales are on it now (in the picture). They were pre-bent for a different model (16' Lund Fury) so I reformed them by hand over the tire of my Volvo L50 loader.
    While reforming they twisted a little so I made a tool to help twist them back into position on top the side wall.
    The tool is made from 1/4" x 3" hot roll and 1 1/4" round tube. I just cut pieces of the 1/4" x 3"to match the gunwale profile and mig welded them together and stuck a handle on it.
    I put one side on the boat first and then hooked a ratchet strap on that one and ran it under the boat to the other gunwale to hold it down while I worked it into place. They're riveted with 3/16" brazier head hard rivets.

    Click image for larger version. 

Name:	15.jpg 
Views:	1470 
Size:	133.6 KB 
ID:	13035Click image for larger version. 

Name:	16.jpg 
Views:	1442 
Size:	127.3 KB 
ID:	13036Click image for larger version. 

Name:	17.jpg 
Views:	1507 
Size:	116.8 KB 
ID:	13037Click image for larger version. 

Name:	18.jpg 
Views:	1487 
Size:	130.4 KB 
ID:	13038

    What's a good source for the polypropylene ? I need 6' x 1' x 1.5".
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  12. #12
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    These guys are local to me, so I get all kinds of stuff from them.

    http://www.iplasticsupply.com/

    They have a huge area of off cuts they sell real cheap, and I can usually find what I need.
    Long arc, short arc, heliarc and in-the-dark!

  13. #13

    Default

    Quote Originally Posted by Rambozo View Post
    These guys are local to me, so I get all kinds of stuff from them.

    http://www.iplasticsupply.com/

    They have a huge area of off cuts they sell real cheap, and I can usually find what I need.
    I like the HDPE but I'd have way too much money in it. The marine plywood was still solid after 35 years so I think I'll go that route.
    I'm putting a new Honda 20hp on it along with a new MotorGuide 36v wireless control trolling motor.
    Last edited by zoama; 07-11-2015 at 10:10 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  14. #14

    Default

    Preparing the floor for 1"x2"x1/8" aluminum stringers to make sure the new 3/16" 5052 deck will feel solid.
    The front area without notches will be raised 12" above the main deck for a livewell, storage and one seat.
    Click image for larger version. 

Name:	19 -.jpg 
Views:	1447 
Size:	141.0 KB 
ID:	13059 Click image for larger version. 

Name:	20.jpg 
Views:	1426 
Size:	132.2 KB 
ID:	13060 Doggie attached to her heatsink as usual.
    Last edited by zoama; 07-19-2015 at 10:47 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  15. #15

    Default

    I haven't worked on the boat in while since my best friend (Doggie) got out of our fenced yard and was killed by a car. I hope to finish the boat this spring.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  16. Default

    Yeah,

    It looks like an elegant design, i.e., no dead spaces, no needlessly used material, there's a dual-purposed cart handle/torch hose rack. Nice.

    One point I'll mention, as I recently modified a Norther Tool welding cabinet to accept two 150 CF bottles, which included ditching the single, loose-fit chain bracket that was well below the centerline of a 150 CF bottle.

    So, maybe it's just a quibble, as two ratchet straps, even below the centerline will undoubtedly secure the bottle well enough, but if I were building a completely custom cart I'd probably have put a couple of uprights and a crossmember at the height of the top of your welder, to secure the bottle above its centerline.


    Quote Originally Posted by zoama View Post
    To the guys who have looked at my cart...

    What would you have done different ?

  17. #17

    Default

    Quote Originally Posted by christian View Post
    Yeah,

    It looks like an elegant design, i.e., no dead spaces, no needlessly used material, there's a dual-purposed cart handle/torch hose rack. Nice.

    One point I'll mention, as I recently modified a Norther Tool welding cabinet to accept two 150 CF bottles, which included ditching the single, loose-fit chain bracket that was well below the centerline of a 150 CF bottle.

    So, maybe it's just a quibble, as two ratchet straps, even below the centerline will undoubtedly secure the bottle well enough, but if I were building a completely custom cart I'd probably have put a couple of uprights and a crossmember at the height of the top of your welder, to secure the bottle above its centerline.
    With the lashing straps pulled tight the bottle is one with the cart. It might as well be welded in. I even shove it sideways by the bottle well above center. No worries
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  18. Default

    I like this cart a lot. Great job!

  19. #19
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by zoama View Post
    What would you have done different ?
    I would probably have built it with a drawer so that consumables etc. are always close at hand.

    My condolences on your loss of Doggie.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  20. Default

    Quote Originally Posted by redbeard View Post
    I would probably have built it with a drawer so that consumables etc. are always close at hand.
    I added a drawer when building mine, and it was definitely worth it. I thought maybe I'd store my helmets in there, but I found it more useful for other misc items like consumables, foot pedal, etc.

    http://www.everlastgenerators.com/fo...ead.php?t=5552
    Everlast welding cart

Similar Threads

  1. Recent Project (250EX) - Welding Cart from Hell
    By Gandalf in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 08-30-2013, 04:42 AM
  2. 250EX-Aluminum welding cart
    By 5440 in forum Other Custom Fabrications
    Replies: 19
    Last Post: 03-25-2013, 10:18 AM
  3. Replies: 13
    Last Post: 03-25-2012, 05:28 PM
  4. First Welding Project - You guessed it... a welding cart
    By EmptyNester in forum Hobyist Projects
    Replies: 19
    Last Post: 10-12-2011, 03:30 PM
  5. Pa200/ PP60 welder cart
    By Scooter in forum Other Custom Fabrications
    Replies: 4
    Last Post: 05-13-2011, 07:15 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •