  1. Default HF vs Blow Back vs HV for plasma table

    I'm looking at plasma cutters for use exclusively in a plasma table (I already have a HT PM45 one for doing free-hand work). I see that most are HF start, and I assume that's the newer technology, but the PP60C is High Voltage start, which I'm not familiar with.

    What are the advantages and disadvantages of each type, specifically when it comes to plasma table work, reliability, and quality of cut?

    For background, I'm looking for a machine that will cut from 14ga to 1/2 inch for the most part, with occasional parts maybe up to 3/4. Seems this is the right range for the PP60C, but is there a unit that would be a better fit?

    Right now I'm sending all this work out, and it's killing me both from cost, but more so, lead time perspective.

    Thanks

  2. #2

    Default

    For 3/4" you are going to need 80 amps for cnc. Blowback will work just fine.

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    HF start can cause interference to the CNC control, so it is prefered to use blowback or high voltage start for CNC. It keeps you from having to shield everything, and having to chase down interference problems. Once cutting, they all cut the same, this is just for starting. Will you use a machine torch or a modified hand torch on your CNC? Also another thing to keep in mind is that if you are using an automatic torch height control, you might have a little more work to do. Everlast has their own voltage divider built in and the values are not what many torch height controls are looking for. Everyone is a little different and there doesn't seem to be a common standard yet.
    Long arc, short arc, heliarc and in-the-dark!

  4. Default

    I will be using a machine torch, thus my preference for the PP60C. Id otherwise be looking at the 80 or 100, but adding another 500 bucks for a machine torch just pushes the budget too far right now.

    After the table is set up and running i`lllook into adding torch height control, but ive read what a hassle integrating one can be, so i`ll tackle that seperately.

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Everlast should think about a "C" version of the newer machines like the 80 and 100 with a machine torch bundle. You can never have too much power for a CNC.
    Long arc, short arc, heliarc and in-the-dark!

  6. #6

    Default

    Quote Originally Posted by Rambozo View Post
    Everlast should think about a "C" version of the newer machines like the 80 and 100 with a machine torch bundle. You can never have too much power for a CNC.
    Funny, I have a 50 in the box (spare) and a 80 we use all the time. I have had a bunch, 50-70, got the 80 and it never left the cart. Power is nice and we freehand with it, normally clean cuts with a good filter.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. plasma data for cnc table use
    By jeverett915 in forum Everlast Plasma Cutters (PAC)
    Replies: 4
    Last Post: 02-18-2016, 04:22 PM
  2. Plasma Table Build - Plasma Bot 4.0
    By SeanMurphy265 in forum Automated welding system (CNC), Submerged ARC, etc.
    Replies: 250
    Last Post: 08-04-2013, 06:05 AM
  3. My DIY Plasma CNC table
    By acourtjester in forum Hobyist Projects
    Replies: 4
    Last Post: 04-16-2013, 07:59 PM
  4. Who has a plasma table?
    By SeanMurphy265 in forum Everlast Plasma Cutters (PAC)
    Replies: 16
    Last Post: 03-27-2012, 12:28 PM
  5. CNC Plasma Table?
    By SeanMurphy265 in forum Everlast Plasma Cutters (PAC)
    Replies: 13
    Last Post: 02-27-2012, 12:37 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •