Quote Originally Posted by Coolidge View Post
I have a new June, 2015 255ext, I just got to test the machine this past weekend and ran into this E04 error. Long story short it was user error in my opinion, contamination of the tungsten. I had a buddy over and we were both running test beads on stainless. Being noobs we dipped the tungsten into the puddle more than once, I had 5 tungsten's on the bench and we were regrinding them throughout the test. The E04 error seemed random until we had cycled through all the tungstens then it wouldn't strike and arc even on a freshly reground tungsten. The issue is I was not regrinding the very tip of the tungsten just the sides. This seemed like a conductivity issue so the next time I got an E04 error I swiped the tip with some 220 grit sandpaper, just scratched it once or twice, bang it struck an arc no problem. So I started grinding about half the tip off the tungsten from there on out after contamination and we never had another E04 error until we again dipped the tungsten into or too close to the puddle and contaminated it. By the way I had the gas up fairly high, 20cfph and was running 6 seconds pre and post flow.

Here's the interesting part. We had been using the water cooled torch with the switch on the torch, which made it a lot more difficult to steady the torch. When we switched to the foot pedal that allowed us a couple three fingers free to steady the torch, we stopped dipping the tungsten into the puddle, maintained a steady stand off, and both the E04 errors and contaminated tungsten issues went away. Hence I'm saying user error in my case.
As you figured out, there can't be a plating of crud on the tip of your tungsten. Also, you typically need less than a second of preflow, so that will help as the arc will start just after you hit the pedal or switch, and not come as a surprise, 6 seconds later. You may need to raise your postflow a little depending on how much current you are using. You want the postflow to last as long as your tungsten is red hot and a little bit more. Otherwise it will pick up some contamination from the air as it cools and can also cause hard starting. When using the torch switch, it sometimes helps to prop the cup on the workpiece, so you can precisely hold the proper arc gap, then hit the switch. That way pressing the switch doesn't cause you to move the torch. Be sure you have a good place to prop your torch hand, too. One of the big keys to good TIG welding is precise torch control.