    The title says it all. I just got my first plasma.....a Power Plasma 60. Had questions about the electrical.....emailed tech support....got the answers i needed. Started setting up the plasma and blew a hose off the inside if the unit......called tech support. Mike told me what to do over the phone to cure the problem.....problem solved. Thursday will be my first day off work since , so i am hoping to play around with the cutter a little. Mike thanks for your help

  2. #2

    Default

    We've had a few blown hoses here and there, not a huge issue, but its a relatively easy fix. We are changing the hose fitting design in the future, but most of the causes of blown hoses are over pressurization. The units should be kept under 90 psi supply. 150 psi compressors will blow them off everytime if they are not regulated at a lower pressure.

  3. Default air pressure

    Thats what wasnt making sense.... the hoses were blowing off at 60 psi. But its all fixed now.... the new clamps are holding fine.

  4. #4

    Default

    Yes, it has happened at lower pressures, but about 80% of the time it is from high pressurization of the line. The clamps are a little temperamental and we will hopefully have that changed in the future, but a 15 cnt hose clamp is all that is required.

  5. #5
    Join Date
    Mar 2011
    Location
    Orlando, Florida
    Posts
    38

    Default

    I keep reading on the svc support and very Impressed!!!!!!!!!!!!!!!!!!!!
    Peter

Similar Threads

  1. Newbie with a Tig
    By slanwar in forum General Welding Questions
    Replies: 7
    Last Post: 02-11-2018, 11:10 PM
  2. Plasma Newbie Everlast 60
    By matkra in forum Introduce Yourself
    Replies: 10
    Last Post: 02-12-2012, 11:51 AM
  3. Newbie from Phoenix
    By ozzy in forum Introduce Yourself
    Replies: 12
    Last Post: 01-25-2012, 06:31 PM
  4. Old Newbie
    By Lone Wolf in forum Introduce Yourself
    Replies: 9
    Last Post: 01-08-2012, 08:25 PM
  5. Newbie on the TIG world
    By Aspen in forum Introduce Yourself
    Replies: 9
    Last Post: 12-09-2009, 06:19 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •