  1. Default Coolant causing sputtering torch

    If you have been following my sputtering torch thread here is the end of it.
    Took out the auto antifreeze and put in distiller water . What do you know my sputter on AC is gone and the torch starts smoother. This was driving me crazy. I can now ramp down to 5amps and still have a steady non sputtering arc. I read somewhere that this could cause hf problems. Made sense that AC welding is basically hf welding. And dc is straight. Hf start on dc have cleaned up tremendously as well.
    Last edited by Chevelle69; 03-08-2015 at 01:47 AM.

Similar Threads

  1. Sputtering in AC mode
    By Chevelle69 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 30
    Last Post: 04-15-2015, 03:30 AM
  2. Tig Cooler Coolant ?
    By Salty in forum TIG Welding (GTAW/GTAW-P)
    Replies: 20
    Last Post: 11-05-2012, 11:31 AM
  3. powercool coolant
    By bigdog35 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 12-05-2011, 08:23 PM
  4. cooler coolant?
    By jdt1986 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 25
    Last Post: 07-22-2011, 10:37 PM
  5. Coolant question
    By Rivets in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 05-04-2011, 02:47 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •