Thread: 200DX/pulse question

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default 200DX/pulse question

    Love the 200DX Tig welder.
    Is it just me, or does it seem that as you come off the pedal mid-weld, you lose the effectiveness of the pulse?
    I'm using a very slow tempo, on the order of 1-1.5pps on some thin aluminum (1/16) and as I'm working my way across and want less heat and roll off the throttle, I just get a steady arc, rather than the hard 'on/off' I had previously. Should the pulse be functional regardless of the pedal position?

    Thanks in advance--
    Chris

  2. #2

    Default

    Since you are using a foot pedal do you have the downslope set to zero?
    Everlast 200DX Dual Voltage
    ThermalArc 181i
    Lincoln ProCut 25
    Victor O/A Torch
    Jackson Pro Variable
    Jackson HSL100 Passive w/Phillips Gold #10
    Tweco Weldskill Auto-Darkening

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by chrispy350 View Post
    Love the 200DX Tig welder.
    Is it just me, or does it seem that as you come off the pedal mid-weld, you lose the effectiveness of the pulse?
    I'm using a very slow tempo, on the order of 1-1.5pps on some thin aluminum (1/16) and as I'm working my way across and want less heat and roll off the throttle, I just get a steady arc, rather than the hard 'on/off' I had previously. Should the pulse be functional regardless of the pedal position?

    Thanks in advance--
    Chris
    Perhaps the pulse amps percentage is the percentage of the panel setting, not what the pedal is set for. So as you lower the output you could fall under that setting and lose pulse. Just a guess, but I know on machines that have a pulse amps instead of pulse percentage, that is what happens. If you are only welding at mid pedal, I can see that being more likely. Try adjusting your max amps so that you can do most of the weld at full pedal, then just back off a little as things heat up. It may be a combination of design and parameters. I'm sure someone from Everlast can supply the details about their pulser design and settings for that machine. Also when you have an issue, it is always helpful to post all your settings.
    Long arc, short arc, heliarc and in-the-dark!

  4. Default 200DX/pulse question

    Thanks guys.
    Yes, I have the slope turned to zero.
    I very much like the explanation that as I use less pedal I'm dropping below the pulse amps threshold, and normalling out.
    Need to continue to find the sweet spot where I get the most pulse control.
    FWIW, I'm using a 3/16 lanthanated tungsten on 1/16 3003 w/ 3/16 1100.
    It's all new metal, so I have the cleaning set to almost minimum on the balance and the freq around 120 or so.
    I'm typically pulsing around 2pps, 50% pulse amps, 75% pulse time.

Similar Threads

  1. 200 DX - Pulse question on AC
    By bmeyer6472 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 09-15-2014, 02:40 AM
  2. 2013 Powertig 200DX 200 Amp 110/220 Dual Voltage Pulse AC/DC
    By magichat in forum TIG Welding (GTAW/GTAW-P)
    Replies: 21
    Last Post: 09-23-2013, 05:22 PM
  3. pulse setting on everlast 200dx
    By steve1989 in forum General Welding Questions
    Replies: 4
    Last Post: 07-31-2013, 06:49 PM
  4. Question re: operation of pulse mode on PowerTig 200DX
    By Tantalum711 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 07-08-2011, 10:21 PM
  5. Power Tig 225LX Pulse Question
    By MikeGyver in forum TIG Welding (GTAW/GTAW-P)
    Replies: 25
    Last Post: 06-15-2011, 01:47 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •