Yet another spray rig, this time on another Kubota RTV900. Took off the stock bed and jigged up a frame for the tank.

Click image for larger version. 

Name:	Weld 047.JPG 
Views:	437 
Size:	146.1 KB 
ID:	12882

I wanted to have some captive nuts for a few things, but I don't have a spot welder to use weldnuts. A couple of options, first for some near the edge of the tube, I used square nuts and drilled a hole on the side for a plug weld. A center drill gave me a nice hole with a 60° chamfer to weld in.

Click image for larger version. 

Name:	Weld 060.JPG 
Views:	428 
Size:	84.3 KB 
ID:	12884 Click image for larger version. 

Name:	Weld 055.JPG 
Views:	457 
Size:	79.3 KB 
ID:	12883

Used for a mounting bracket for an engine/pump.

Click image for larger version. 

Name:	Weld 062.JPG 
Views:	420 
Size:	107.0 KB 
ID:	12885 Click image for larger version. 

Name:	Weld 071.JPG 
Views:	449 
Size:	116.6 KB 
ID:	12886

For some in the center of a tube, I used a flange nut and drilled the hole next to the bolt hole, for the plug weld.

Click image for larger version. 

Name:	Weld 077.JPG 
Views:	431 
Size:	81.6 KB 
ID:	12887 Click image for larger version. 

Name:	Weld 079.JPG 
Views:	424 
Size:	97.1 KB 
ID:	12888

Welding up the frame. A mixture of MIG and TIG.

Click image for larger version. 

Name:	Weld 082.JPG 
Views:	452 
Size:	139.1 KB 
ID:	12889

Primed and ready to send out for paint?

Click image for larger version. 

Name:	Weld 088.JPG 
Views:	432 
Size:	128.9 KB 
ID:	12890

Painter didn't show up, so the boss went at it with a brush.