First of all i should say, I love this machine. Once im up and running and dialed in this little machine makes the most amazing sizzles sounds ever, smooth as silk. Has made me on occasion look like a much better welder than I actually am.
On to my question / problem. I have a lot of problems getting the arc started. I've tried tapping and scratching, both techniques give about the same frustrating results: sticking! I generally use 7018 1/8" Rod.
Most of the welding I do is generally related to repair of skid steer attatchments.
I clean and prep my weld area usually with wire wheel. Same with ground, i wire wheel to a clean surface. I tend to weld a little hotter than I should, as this machine generally amazes me with the power it has to spare. I also try and clean the ground clamp reasonably close to where I am welding.
Would swapping to something other than 7018 help me out? I've got 7014 and 6011 on hand, but i generally default to 7018 since it can consistantly deliver beautiful looking welds. Would larger cables help me out somehow? Any sort of suggestions appreciated.




Reply With Quote