Hi,
I'm sort of starting to get the hang of 6010 at school and was hoping to duplicate (at least somewhat) the results I'm getting at school with my 210EXT. I'm got the arc force set at about 60%, I've got the VRD turned off. I've tried AC, DCEP, DCEN but I'm not getting the same results that I'm getting with the schools big machines. They have 300-400 amp machines that are about half the size of a refrigerator. I was hoping to get 6011 working somewhat similar to the 6010 we are using at school. My biggest problem is getting the arc to stay lit, it goes out when I 'whip' it up (inverted T). I've got a real forceful arc, but it's not acting the same.
I'm happy with the TIG part of the machine, but I'm having problems with the stick part.




Reply With Quote