  1. Default no post flow (210 ext)

    Ive had my powertig 210 ext for a year or two now and it has worked great till recently. I started noticing there was no post flow after ending a weld. I checked my settings it was set for 9 sec. of post flow. It does it in ac and dc modes and it seems like when i have the foot pedal to the floor and release it real quick i get post flow about 75% of the time it doesnt all ways work. has anyone else had this problem ?

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Have you tried changing the post flow setting? Maybe run it to zero, cycle it a few times, and then reset it to the desired time, and see if that clears things out. I don't think there is a software reset on that machine, but it wouldn't hurt to give tech support a call. They might have a solution for you.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    Yes, give tech support a call at ext 207. It could be your pedal isn't returning all the way to off.

  4. Default

    I unplugged the foot pedal and plugged in the torch switch and it worked fine , so i called tech support and ray said send it in its probably something in the machine.

  5. #5

    Default

    Still sounds like pedal to me. Did you check it with an ohm meter to see if when you let up slow is pin 1-3 opening up? Ray's the man, but I would check that.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by everlastsupport View Post
    Still sounds like pedal to me. Did you check it with an ohm meter to see if when you let up slow is pin 1-2 opening up? Ray's the man, but I would check that.
    Wouldn't that give something like a never ending post flow? From what he says, it sounds like the argon flow stops right away. But for sure with it working with the torch switch and not with the pedal, I would thoroughly check out the pedal for all wiring and values, before sending the whole unit in.
    Long arc, short arc, heliarc and in-the-dark!

  7. Default

    do you have the pin out handy ?

  8. #8
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by kelly8969 View Post
    do you have the pin out handy ?
    Quote Originally Posted by everlastsupport View Post
    The 210EXT foot pedal pinout is:

    1 - 3 is the trigger switch

    5 - 2 is 10-1K ohms

    5 - 4 is 1K to 10 ohms
    This is from a previous post in the Technical section. You can find most of the pinouts there.
    Long arc, short arc, heliarc and in-the-dark!

  9. #9

    Default

    Quote Originally Posted by Rambozo View Post
    Wouldn't that give something like a never ending post flow? From what he says, it sounds like the argon flow stops right away. But for sure with it working with the torch switch and not with the pedal, I would thoroughly check out the pedal for all wiring and values, before sending the whole unit in.
    No, the releasing it real quick sounds like a malfunctioning switch which triggers the post flow cycle when it is recycled.

Similar Threads

  1. Post flow will not stop,and cannot adjust amps just stays on 45
    By Mickhd in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 6
    Last Post: 04-29-2014, 12:14 PM
  2. I-Tig 200 post flow "stuck"?
    By Zacho in forum General Welder Questions
    Replies: 3
    Last Post: 05-18-2011, 05:19 PM
  3. Power Plasma 50 Post Flow Air Question
    By cpierce18 in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 06-28-2010, 03:02 PM
  4. post flow timer/gas valve?
    By Doug Wright in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 03-22-2010, 08:11 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •