    Do you mind clarifying this sentence:

    Quote Originally Posted by drthunder33 View Post
    ...and some of the truck parts I deal with may not be ideal (clean) for mig.
    Are you saying the truck parts may not be clean? If so, (and I don't mean to preach) you should know TIG requires VERY clean weld materials, down to bright shiny metal and any surface contaminants removed prior to welding. Did I get your question right, or did I miss something?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  2. #2

    Default

    Sorry, to clarify, the trucks are "mud trucks" and there may be some rust and paint at the repair/ modification area. I have no immediate plans for tig welding but I do plan on using the stick feature with some 6010 to bust through any possible contaminants.

    Thanks for the info. I'm kinda new to all this so all the help I can get is more than appreciated.
    .

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Just a couple of points, You might want to check about the mutiprocess machine and 6010. I do not believe they work well with that rod. If you use 6011 you should be ok, but if you must have 6010, you probably want to get an inverter that has a specific 6010 rating. Also the multiprocess machines are not recommended for CNC or other extended operation like your pantograph, because that kind of operation will often max out the duty cycle. There is a thread here a few years back where rodsmachine rigged up a simple 1:1 tracer for a plasma. A pantograph would be even better as a poorman's CNC. You might also look at MIG/Stick combos, since that sounds like the kind of work you do. Then add a dedicated plasma and you will be good to go, even if you upgrade later to a CNC.
    Long arc, short arc, heliarc and in-the-dark!

  4. #4

    Default

    Rambozo is right. The MP unit is more of a weekend warrior, light work machine. A machine driving it (CNC) would kill it in no time. I would go dedicated MIG and Plasma. We (my places) have a PP80 and MIG250 for shop work and a IMIG 200 for on the road, also a PP50 but plasma draw a lot of current so a bigger generator is required.

    If you need to TIG and have a budget the PT185 down the road. We do steel and aluminum with the little IMG 200. I would look at that machine. A lot of people like the new MIG140, based on price point and power. If you need 6010, look at the Power Arc line, but stick only.

    Mark can tell you what machines for 6010, I would just use 6011 since you are just mudding,
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. #5

    Default

    The duty cycles between the pp50 and pu205 seem to be the same at 240v. Am I missing another parameter that makes the pp50 a better cutter?

  6. #6

    Default

    Quote Originally Posted by drthunder33 View Post
    The duty cycles between the pp50 and pu205 seem to be the same at 240v. Am I missing another parameter that makes the pp50 a better cutter?
    Output drivers are better. The PP50 you can abuse, tough IGBTs. Also, the PP50 only powers a plasma circuit. The pu205 powers a welder(TIG/MMA) and plasma circuit.

    Also, PU205 is a TIG and plasma, not a MIG and plasma, like DaveO pointed out. If you want to weld fast and dirty, that's MIG or stick. PU205 will work if you want MMA/Stick and that is why Ram mentioned 6010 and 6011.

    Heck, now I'm confused...

    I would go with dedicated machines, though more money. My vote, IMIG200, PP50. Later PT185. I have not used the 140, but getting one, it might be all you need.

    We (personally) have too many mud trucks and trailers, quads, UTVs, golf carts.. MIG and plasma to start, it will do what you need.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. #7
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by everlastsupport View Post
    Output drivers are better. The PP50 you can abuse, tough IGBTs. Also, the PP50 only powers a plasma circuit. The pu205 powers a welder(TIG/MMA) and plasma circuit.

    Also, PU205 is a TIG and plasma, not a MIG and plasma, like DaveO pointed out. If you want to weld fast and dirty, that's MIG. PU205 will work if you want MMA/Stick and that is why Ram mentioned 6010 and 6011.

    Heck, now I am confused...
    I was thinking along the lines of something like an iMIG 200 or better, to give you 6011 stick and MIG, a great one two punch for repairs and off-road fab. Then pair it up with a plasma that could be used manually, or on a pantograph and could also be used on a future CNC project.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. Why is there only Multi Process or MIG/TIG/Stick?
    By jp2code in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 6
    Last Post: 02-21-2012, 04:50 PM
  2. Tip for Multi-process machine users
    By dirtyfarmer in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 04-09-2011, 05:29 AM
  3. Multi Process and torch cooler
    By Tony_F in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 04-23-2010, 01:18 PM
  4. pure plasma or multi process?
    By alexm in forum General Welder Questions
    Replies: 8
    Last Post: 01-27-2010, 02:43 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •