  1. Default Help...Tungsten Balling?

    I have the PP205 and haven't typically had any issues with my Tungsten Balling on DC. I have been welding 1/8" steel plate at a max of about 125-140 amps with straight Argon at 10 l/min. Preflow at about 3 seconds and post flow at 7 seconds or so. 1/8" Lanthanated electrode and I was using #5 cup and switched to a #7 cup to hope let more gas flow. Tungsten still starts to ball after about 1 minute of welding.

    Does anyone have a diagnosis and a remedy?

    Thanks in advance for any help!!

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Are you sure you don't have the leads swapped? Torch should be in negative. It takes a lot to ball an 1/8"
    Long arc, short arc, heliarc and in-the-dark!

  3. Default

    That's what I thought. Torch leads are correct. thanks.

  4. #4

    Default

    Is the arc quiet like DC should be ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. Default

    Yes it is. Thanks..

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Does the tungsten stay bright and shiny or does it get grey and blistered?

    Out of curiosity you could try swapping the leads and see how it behaves.
    Last edited by Rambozo; 01-18-2015 at 11:58 PM.
    Long arc, short arc, heliarc and in-the-dark!

  7. Default

    The tungsten use to get dirty and black at 7 l/min argon, so I increased to 10 l/min argon and measured with a metered device at the tungsten (not sure what it is called, but looks like a little breaker with a bb in it to measure gas flow at the torch) and the tungsten now stays shiny. Thanks for your input.

  8. #8

    Default

    If that is the flow meter that came with your unit, that is not for the TIG torch. It is for the plasma. Won't work.

  9. Default

    It's not. I bought the flow meter specifically to measure flow at my TIG torch. Thanks.

  10. #10
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Well if it is staying clean, it's probably not a gas issue. The only thing left is somehow you have a substantial DCEP component going on there. Did you ever try swapping the leads?
    Long arc, short arc, heliarc and in-the-dark!

  11. Default

    not yet. I will try next weekend. Thanks for your help.

Similar Threads

  1. Tungsten balling up, what's wrong
    By diyjer in forum TIG Welding (GTAW/GTAW-P)
    Replies: 45
    Last Post: 09-01-2022, 01:16 AM
  2. Smallest Tungsten you use?
    By CGCINC in forum TIG Welding (GTAW/GTAW-P)
    Replies: 17
    Last Post: 06-27-2012, 03:03 AM
  3. Tungsten
    By bigjoeinkg in forum General Welding Questions
    Replies: 5
    Last Post: 08-29-2011, 01:17 AM
  4. Tungsten Grinder
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 07-22-2011, 01:03 AM
  5. tungsten grinder
    By gwk in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 03-13-2011, 01:02 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •