Share
Results 1 to 4 of 4

Thread: Help noob with aluminum

Threaded View

Previous Post Previous Post   Next Post Next Post
  1. Default Help noob with aluminum

    I recently purchased a power tig 200dx. I've managed to get the hang of welding steel and even welded some copper, but I am having a terrible time with aluminum. I am just trying to put some beads on some 1/8" flat bar but it just isn't working. As soon as I get it hot enough to get a puddle or melt the filler rod it simply melts a hole through the material. I've tried different settings with the frequency and AC balance but it is always the same result. I have adjusted the gas flow and cleaned and re-cleaned the material with no success. I have attached photos of the top and bottom of the bar. The bubbled side is the bottom. Please help if possible.

    Thanks,

    Forrest
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	DSC_0332.jpg 
Views:	472 
Size:	47.1 KB 
ID:	12736   Click image for larger version. 

Name:	DSC_0335.jpg 
Views:	466 
Size:	39.6 KB 
ID:	12737  

Similar Threads

  1. Everlast PowerPro205-Noob that can't weld aluminum. Please help!
    By T_Money in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 06-27-2013, 04:06 AM
  2. Noob in need of help
    By Chuck_jkl in forum Introduce Yourself
    Replies: 10
    Last Post: 01-24-2013, 02:17 AM
  3. noob
    By bubbas55 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 11-08-2012, 01:23 AM
  4. PowerTig 200LX Aluminum noob pics
    By Mad-Dax in forum Hobyist Projects
    Replies: 29
    Last Post: 04-15-2012, 10:26 PM
  5. Noob to Tig
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 04-06-2011, 04:46 AM