    Should the ball in the regulator aways be floating even when not welding?

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Hypnotk View Post
    Should the ball in the regulator aways be floating even when not welding?
    No. After any post flow the ball should drop to the bottom. If it doesn't, you have a leak.
    Long arc, short arc, heliarc and in-the-dark!

  3. Default

    Hmmmm....then i have a leak. Thank you.

Similar Threads

  1. Quick gas question 255EXT
    By Gusman in forum TIG Welding (GTAW/GTAW-P)
    Replies: 10
    Last Post: 08-17-2017, 12:09 AM
  2. Quick question about grounding a 250 ex
    By Blaze in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 07-21-2016, 11:17 PM
  3. Quick question regarding Powerplasma 50
    By Rupes in forum Everlast Plasma Cutters (PAC)
    Replies: 8
    Last Post: 03-29-2014, 05:22 PM
  4. Quick question, need some help?
    By CGCINC in forum General Welding Questions
    Replies: 11
    Last Post: 07-04-2012, 05:02 PM
  5. Question about Pre-Flow.
    By brianscott in forum General Welding Questions
    Replies: 4
    Last Post: 01-12-2012, 09:35 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •