Thread: my power pro exploded

  1. Exclamation my power pro exploded

    while trying to use the plasma cutter i noticed the whole machine tripped out, i unplugged the leads and tryed to restart and thought someone had shot a 9mm ,it had tripped again. i blow dry air in it thinking it may be a moisture issue and tried it again this time it came on for just a minute then tripped out again.took the cover off and found a burnt spot on left side. this machine is only a year and 3 months old.can a everlast tech please help i dont want to loose my welder for a month or three due to shipping.hoping to fix myself with some guidenceClick image for larger version. 

Name:	vacation 2014 everlast carleys birth 163.jpg 
Views:	523 
Size:	143.1 KB 
ID:	12643Click image for larger version. 

Name:	vacation 2014 everlast carleys birth 164.jpg 
Views:	539 
Size:	146.8 KB 
ID:	12644Click image for larger version. 

Name:	vacation 2014 everlast carleys birth 165.jpg 
Views:	481 
Size:	139.7 KB 
ID:	12645Click image for larger version. 

Name:	vacation 2014 everlast carleys birth 168.jpg 
Views:	490 
Size:	127.2 KB 
ID:	12646Click image for larger version. 

Name:	vacation 2014 everlast carleys birth 166.jpg 
Views:	468 
Size:	150.5 KB 
ID:	12647

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Vaporized that resistor completely.
    Long arc, short arc, heliarc and in-the-dark!

  3. Default

    yeah it was laying in the bottom of the welder

  4. Default

    But realize, that resistor isn't the problem, it's a symptom so, don't just go replacing it...

    Too much current was flowing through the resistor for a reason, you gotta find-out what that reason was for it to be "fixed"!

  5. #5

    Default

    Yeah, That's something you'll need to send in. Not much to say otherwise than I hate it happened, but that's why I don't recommend them for the average user. Portable repair and factory maintenance yes. That's the plasma side of the board definitely.

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Long arc, short arc, heliarc and in-the-dark!

  7. Default

    that was NOT funny ok it was

  8. #8

    Default

    I am not sure what causes that to happen other than something hung? Mike may be able to explain it better than I can. Ray probably knows, but he seldom gets to check in these days. The 205S is pretty stable.

    Anything particular you were doing when it happened? Don't worry, whatever was should be covered under warranty.

  9. #9

    Default

    Quote Originally Posted by performance View Post
    I am not sure what causes that to happen other than something hung? Mike may be able to explain it better than I can. Ray probably knows, but he seldom gets to check in these days. The 205S is pretty stable.

    Anything particular you were doing when it happened? Don't worry, whatever was should be covered under warranty.
    Mark's right, probably an IGBT latched up. Routed all that power to the poor little resistor. But it will need to come in for repair. A lot of times, it takes them all out, though there was only a burn in the one spot.

    Call in for Ray for an RMA #. Not something that can be fixed in the field.

    Funny, I recall that clip from back when I was a kid...
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  10. Default

    ok,ill call ray weds morning. thanks for the imput,guess you cant win them all but thank yall very much

Similar Threads

  1. Power Pro 256 power on issue
    By wheelrdealer in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 02-27-2019, 02:47 AM
  2. Power Tig 250EX Power Cord Connections
    By Chris411968 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 01-31-2010, 06:58 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •