Hey, I'm new to the forums. I have a procut50 and it's blue it stead of green?... I'm guessing it's pretty much the same as the supercut 50. I was wondering about swapping the torches out for one that has a trigger instead of the button on top. It's set up just like the super cut. Threaded lead with air through, 2 pin switch, and the pilot arc stud on the front. Are there any compatible torches?