    I tried welding up a rod holder(fishing pole) from 3/8" solid bar and it seems to work fine on heavy stuff. At least the blast didn't seem to affect anything, using both button and foot.

    I have some 3/16" brazing rods I want to put in to fill some of the spaces. This is a rough example of what I'm thinking of. How do you weld them to SS?

    Charlie

    Everlast 225 LX
    Everlast PP 50

    HF 130 TIG/90 ARC
    HF 90 fluxcore

    ATX MIG (don't ask)

  2. #2

    Default

    You can't weld brass to SS. You can braze it with O/A or low amp tig, but the two metals are incompatible. You'd end up melting the pieces of rod though and you'd need flux.

Similar Threads

  1. First run (with some problems) - Power Tig 225lx
    By marcio in forum TIG Welding (GTAW/GTAW-P)
    Replies: 12
    Last Post: 03-14-2013, 01:26 AM
  2. My new 225lx
    By dyethor in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 02-24-2012, 07:00 AM
  3. 225LX can't seem to get it to tig..
    By Hayapower in forum TIG Welding (GTAW/GTAW-P)
    Replies: 19
    Last Post: 12-10-2011, 12:57 AM
  4. Just got my 225LX and tried it out
    By DiabolicZ in forum TIG Welding (GTAW/GTAW-P)
    Replies: 29
    Last Post: 04-02-2011, 08:01 PM
  5. My 225LX is here
    By dgeese in forum Customer Testimonials
    Replies: 4
    Last Post: 01-03-2011, 11:07 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •