I tried welding up a rod holder(fishing pole) from 3/8" solid bar and it seems to work fine on heavy stuff. At least the blast didn't seem to affect anything, using both button and foot.

I have some 3/16" brazing rods I want to put in to fill some of the spaces. This is a rough example of what I'm thinking of. How do you weld them to SS?