  1. Default a few problems?

    Hi guys I'm having a few issues with my 230ex (Aust) Where I have the pulse turned off and after a few welds its starting to pulse ( numbers are going up and down)? Once I reset the switch to the off pozzie its stops? Also I'm getting small zaps though the handle sometimes when I'm welding. Is this normal?

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    High Frequency current during starts can leak through some cables and torch parts, especially if they are dirty. Also if your gloves have soaked up sweat, that provides a good path for HF. Each person has different perceptions of feeling that, too. Some notice small leaks much more than others. Check to make sure everything is clean and dry. You can wash the handle and torch body with alcohol, or soap and water, but avoid stronger solvents.
    Not sure about the pulsing, maybe someone else can point you in the right direction of what can cause that.
    Long arc, short arc, heliarc and in-the-dark!

  3. Default

    cheers for that I'll give cleaning the torch a go, also I 've got some 2.4mm tungsten and rods and cant get an arc started just little zapping noises and current between torch and surface??

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by nikstiks View Post
    cheers for that I'll give cleaning the torch a go, also I 've got some 2.4mm tungsten and rods and cant get an arc started just little zapping noises and current between torch and surface??
    That sounds like a bad ground. HF will jump the gap even without a good ground, but the main arc will not transfer.
    Long arc, short arc, heliarc and in-the-dark!

  5. Default

    cheers will try again

Similar Threads

  1. Seriously?! (NEW 51-P problems)
    By tdkask in forum Everlast Plasma Cutters (PAC)
    Replies: 5
    Last Post: 05-25-2016, 11:43 PM
  2. PP205 problems--
    By JBnID in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 0
    Last Post: 08-23-2014, 06:21 PM
  3. 250 ex problems
    By johnson697 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 07-04-2013, 10:44 AM
  4. Plasma Problems
    By Slartybartfa in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 34
    Last Post: 07-03-2012, 02:03 AM
  5. MIG 200 tip problems
    By countrygardener in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 7
    Last Post: 11-08-2010, 08:47 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •