Yea,,, I don't like that 666 stuff at ALL....

My 256 did some really weird stuff when the Pedal Connector, on the machine, was not tight. It Maxed-Out as soon as the switch was tripped and acted like I didn't have a pedal connected. Tightening the connector ring and it went back to normal.