    I just bought a I-mig 200e and im still waiting for it to arrive via ups. Just wanting to see peoples opinions on this machine. Not sure if this model has been out long at all. Im brand new to the everlast brand

  2. #2
    Join Date
    Aug 2014
    Location
    Trenton, New Jersey, United States
    Posts
    263

    Default

    Hello. I don't have a 200E. But do have the "Little Brother" to it. The 140E. As I only have a 120V outlet. Like you I am a New Owner. So far the only issue I have had is with some of the Consumables. As they need to come from Everlast directly. Have not been able to locate a Dealer locally. I love that I can use it constantly without tripping the Protection circuits. Or even the 20A breaker. It runs pretty quiet.

  3. #3

    Default

    No, you don't need to get consumables directly from us. As far as the gas nozzles/cones, there are multiple sources locally and online. Northern Tool, Harbor Freight, and TSC are common places you can buy them. You can also get them from places like Snapon, Matco or other places as they all use the same guns. HTP and Clarke and a whole bunch use this. The consumables are available from many online retailers such as HTP, welding direct(under Nutech name), river-weld.com, and many others. Many local welding suppliers are either binzel or trafimet dealers and you can get them from there as well. The Tips are standard TWECO tips and are available from almost any welding supply store or Home Depot or Lowes as they fit Lincoln too.

  4. #4
    Join Date
    Aug 2014
    Location
    Trenton, New Jersey, United States
    Posts
    263

    Default

    Thanks Mark. My local dealers only deal with the "Three Kings". I did find a Spot Weld nozzle for the 15AK torch on Ebay. What I should have said was some parts. FC Drive Roller for example. When I can, I am getting the 3M Torch. The 2M is awkward to work with.

  5. #5

    Default

    They may be dealing in name brand welders but that has nothing to do with the torches they sell or service. A lot of companies sell other brands of torches according to the customer tastes...that aren't OEM equipment. They have aftermarket suppliers so they customers can have a wide range of options.

  6. #6
    Join Date
    Aug 2014
    Location
    Trenton, New Jersey, United States
    Posts
    263

    Default

    I Apologize for "Hijacking" your thread.

    My local shops have a bit of an Attitude about "Chinese" welders. They're very little help. I need to see the nicer guy for a refill of my Argon/C25. Down to about 300 PSI. Have enough for the bracket(Mentioned in a different Thread) if needed.

  7. #7
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    The best thing to do is just to bring in the parts you need and match them up. You can swap with Bernard, Tweco, Binzel, Profax, Trafimet, etc. Don't even bother going in and asking about parts for Everlast. It's all about the actual MIG gun, not the power supply, and a ton of those parts are standard and interchange. You would get the same thing if you tried to get parts for a 20 year old Millermatic. Who knows what came as an original gun and what it was replaced with. Many big name welders were sold without a gun, and that was purchased as a separate item from a different maker. Just bring in your old parts and match them up, and I'm pretty sure they will have bits that will work for you. If you want, you can make a note of the part numbers for next time.
    Long arc, short arc, heliarc and in-the-dark!

  8. #8

    Default

    Ram is right. Take them in and they will match them as long as not too mangled. You will find you can go to Harbor Freight for the electrodes and nozzles as well, but most LWS will fix you up and it's all about the torch. Bring torch is as well.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  9. #9

    Default

    Come to think of it, the Miller Cricket and another Miller unit (can't remember right now) used the same gun a ways back.

Similar Threads

  1. 10lb spool in 200e
    By dsthompson in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 1
    Last Post: 04-15-2018, 04:31 AM
  2. I-MIG 200E- is this real?
    By drthunder33 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 2
    Last Post: 02-11-2015, 03:39 PM
  3. I-MIG 200E, What do I need with it?
    By drthunder33 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 1
    Last Post: 01-21-2015, 08:35 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •