    Doing some cutting on the torchmate tonightClick image for larger version. 

Name:	image.jpg 
Views:	539 
Size:	148.0 KB 
ID:	12474Click image for larger version. 

Name:	image.jpg 
Views:	537 
Size:	146.1 KB 
ID:	12475Click image for larger version. 

Name:	image.jpg 
Views:	537 
Size:	143.6 KB 
ID:	12476Click image for larger version. 

Name:	image.jpg 
Views:	545 
Size:	144.8 KB 
ID:	12477Click image for larger version. 

Name:	image.jpg 
Views:	505 
Size:	146.8 KB 
ID:	12478Click image for larger version. 

Name:	image.jpg 
Views:	539 
Size:	148.0 KB 
ID:	12474Click image for larger version. 

Name:	image.jpg 
Views:	537 
Size:	146.1 KB 
ID:	12475Click image for larger version. 

Name:	image.jpg 
Views:	537 
Size:	143.6 KB 
ID:	12476
    Machines: EVERLAST Power Tig 210EXT w/ water cooler and 25' CS310 weldcraft torch
    LONGEVITY 250EX Tig
    MILLER 211 mig w/spool gun
    EVERLAST Power Plasma 80s mounted on my Torchmate 2x2 cnc table
    SMITHY 1324 mill/lathe
    60 gal. 7.5 hp air compressor


    MY YOUTUBE CHANNEL: https://www.youtube.com/user/dzljon/videos

  2. #2

    Default

    Very nice. How bad was the cleanup? It is nice you can make your own parts. Did torchmate come with controller and software?
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. #3

    Default

    That's really good work. Oleg forwarded me pictures of that last you night. If you can, post up the consumable size, material thickness, amp used, thc or not, speed etc. and the details about what it is and why it's needed ( for conversion I believe) for others reading interest.

    IF you can swing it, I'd suggest getting the machine torch as performance should be better.

  4. #4

    Default

    Quote Originally Posted by everlastsupport View Post
    Very nice. How bad was the cleanup? It is nice you can make your own parts. Did torchmate come with controller and software?
    Thanks! The torchmate came with everything but the computer and cutter.
    Machines: EVERLAST Power Tig 210EXT w/ water cooler and 25' CS310 weldcraft torch
    LONGEVITY 250EX Tig
    MILLER 211 mig w/spool gun
    EVERLAST Power Plasma 80s mounted on my Torchmate 2x2 cnc table
    SMITHY 1324 mill/lathe
    60 gal. 7.5 hp air compressor


    MY YOUTUBE CHANNEL: https://www.youtube.com/user/dzljon/videos

  5. #5

    Default

    Quote Originally Posted by performance View Post
    That's really good work. Oleg forwarded me pictures of that last you night. If you can, post up the consumable size, material thickness, amp used, thc or not, speed etc. and the details about what it is and why it's needed ( for conversion I believe) for others reading interest.

    IF you can swing it, I'd suggest getting the machine torch as performance should be better.
    This part allows the factory tach in ford trucks work with a cummins engine, metal is 3/16, cut rate was 40 ipm, at 45 amps, no torch height control, consumables are 1.0 tip for the s75 torch. I am looking to getthe machine torch in the future. Thank you for the questions.
    Machines: EVERLAST Power Tig 210EXT w/ water cooler and 25' CS310 weldcraft torch
    LONGEVITY 250EX Tig
    MILLER 211 mig w/spool gun
    EVERLAST Power Plasma 80s mounted on my Torchmate 2x2 cnc table
    SMITHY 1324 mill/lathe
    60 gal. 7.5 hp air compressor


    MY YOUTUBE CHANNEL: https://www.youtube.com/user/dzljon/videos

  6. #6
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Very impressive work. After cutting and clean up did you have to balance it, like you would for a boat prop?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  7. #7

    Default

    Quote Originally Posted by dzljon View Post
    Thanks! The torchmate came with everything but the computer and cutter.
    What's the price ? I couldn't find any pricing at their website.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  8. #8

    Default

    Quote Originally Posted by DaveO View Post
    Very impressive work. After cutting and clean up did you have to balance it, like you would for a boat prop?
    Thanks!No balanceing required for this applcation
    Machines: EVERLAST Power Tig 210EXT w/ water cooler and 25' CS310 weldcraft torch
    LONGEVITY 250EX Tig
    MILLER 211 mig w/spool gun
    EVERLAST Power Plasma 80s mounted on my Torchmate 2x2 cnc table
    SMITHY 1324 mill/lathe
    60 gal. 7.5 hp air compressor


    MY YOUTUBE CHANNEL: https://www.youtube.com/user/dzljon/videos

  9. #9

    Default

    Quote Originally Posted by zoama View Post
    What's the price ? I couldn't find any pricing at their website.
    Best thing to doi s give them a call, because of all the options prices a different
    Machines: EVERLAST Power Tig 210EXT w/ water cooler and 25' CS310 weldcraft torch
    LONGEVITY 250EX Tig
    MILLER 211 mig w/spool gun
    EVERLAST Power Plasma 80s mounted on my Torchmate 2x2 cnc table
    SMITHY 1324 mill/lathe
    60 gal. 7.5 hp air compressor


    MY YOUTUBE CHANNEL: https://www.youtube.com/user/dzljon/videos

  10. #10

    Default

    Quote Originally Posted by dzljon View Post
    Thanks! The torchmate came with everything but the computer and cutter.
    Was the the part was in their library or on the net? How was the learning curve on the software?
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  11. #11

    Default

    Quote Originally Posted by everlastsupport View Post
    Was the the part was in their library or on the net? How was the learning curve on the software?
    i had to draw the whole part, spent about 45 minutes drawing it and about 3 minutes cutting each one, the soft ware is pretty easy ince you rap your mind around the terminology, but they have a awsome customer support center to help you with any issues, or questions, thye know the machines and software very well
    Machines: EVERLAST Power Tig 210EXT w/ water cooler and 25' CS310 weldcraft torch
    LONGEVITY 250EX Tig
    MILLER 211 mig w/spool gun
    EVERLAST Power Plasma 80s mounted on my Torchmate 2x2 cnc table
    SMITHY 1324 mill/lathe
    60 gal. 7.5 hp air compressor


    MY YOUTUBE CHANNEL: https://www.youtube.com/user/dzljon/videos

  12. #12

    Default

    Quote Originally Posted by dzljon View Post
    i had to draw the whole part, spent about 45 minutes drawing it and about 3 minutes cutting each one, the soft ware is pretty easy ince you rap your mind around the terminology, but they have a awsome customer support center to help you with any issues, or questions, thye know the machines and software very well
    Pretty slick. So you drew it in their cad/editor. And then sent it to cut? If so, slick. So you added computer and plasma cutter and you were running? How bad was assembly? I looked at the 2x2 but never bought. Sounds like it was pretty straight forward.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  13. #13

    Default

    Click image for larger version. 

Name:	image.jpg 
Views:	475 
Size:	145.1 KB 
ID:	12484Click image for larger version. 

Name:	image.jpg 
Views:	476 
Size:	107.6 KB 
ID:	12483

    This is my work space for plasma cutting
    Last edited by dzljon; 10-31-2014 at 05:46 PM.
    Machines: EVERLAST Power Tig 210EXT w/ water cooler and 25' CS310 weldcraft torch
    LONGEVITY 250EX Tig
    MILLER 211 mig w/spool gun
    EVERLAST Power Plasma 80s mounted on my Torchmate 2x2 cnc table
    SMITHY 1324 mill/lathe
    60 gal. 7.5 hp air compressor


    MY YOUTUBE CHANNEL: https://www.youtube.com/user/dzljon/videos

  14. #14

    Default

    That would work for me.. Little tight but nice, that is how we work here. So the software was not too bad, or their support is really good. is that a 2x4? Mind PMing price breakdown LOL. Nice thing is, over time it will pay for itself.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  15. #15

    Default

    Cut 1/2" at 20 ipmClick image for larger version. 

Name:	image.jpg 
Views:	518 
Size:	148.1 KB 
ID:	12497Click image for larger version. 

Name:	image.jpg 
Views:	483 
Size:	144.9 KB 
ID:	12498Click image for larger version. 

Name:	image.jpg 
Views:	473 
Size:	146.4 KB 
ID:	12499
    Machines: EVERLAST Power Tig 210EXT w/ water cooler and 25' CS310 weldcraft torch
    LONGEVITY 250EX Tig
    MILLER 211 mig w/spool gun
    EVERLAST Power Plasma 80s mounted on my Torchmate 2x2 cnc table
    SMITHY 1324 mill/lathe
    60 gal. 7.5 hp air compressor


    MY YOUTUBE CHANNEL: https://www.youtube.com/user/dzljon/videos

  16. #16

    Default

    Close up on 3/16
    Click image for larger version. 

Name:	ImageUploadedByTapatalk1417313265.744335.jpg 
Views:	472 
Size:	15.6 KB 
ID:	12613
    Click image for larger version. 

Name:	ImageUploadedByTapatalk1417313284.063447.jpg 
Views:	452 
Size:	15.5 KB 
ID:	12614


    Sent from my iPhone using Tapatalk
    Machines: EVERLAST Power Tig 210EXT w/ water cooler and 25' CS310 weldcraft torch
    LONGEVITY 250EX Tig
    MILLER 211 mig w/spool gun
    EVERLAST Power Plasma 80s mounted on my Torchmate 2x2 cnc table
    SMITHY 1324 mill/lathe
    60 gal. 7.5 hp air compressor


    MY YOUTUBE CHANNEL: https://www.youtube.com/user/dzljon/videos

  17. #17

    Default

    Click image for larger version. 

Name:	ImageUploadedByTapatalk1417313341.231963.jpg 
Views:	445 
Size:	10.7 KB 
ID:	12615
    3/16 sheet used on my caster wheel project


    Sent from my iPhone using Tapatalk
    Machines: EVERLAST Power Tig 210EXT w/ water cooler and 25' CS310 weldcraft torch
    LONGEVITY 250EX Tig
    MILLER 211 mig w/spool gun
    EVERLAST Power Plasma 80s mounted on my Torchmate 2x2 cnc table
    SMITHY 1324 mill/lathe
    60 gal. 7.5 hp air compressor


    MY YOUTUBE CHANNEL: https://www.youtube.com/user/dzljon/videos

  18. #18

    Default PP 80s on a torchmate

    This is a biocide and corrosion fighter for the plasma water table
    Click image for larger version. 

Name:	ImageUploadedByTapatalk1419877656.760761.jpg 
Views:	428 
Size:	14.6 KB 
ID:	12717


    Sent from my iPhone using Tapatalk
    Machines: EVERLAST Power Tig 210EXT w/ water cooler and 25' CS310 weldcraft torch
    LONGEVITY 250EX Tig
    MILLER 211 mig w/spool gun
    EVERLAST Power Plasma 80s mounted on my Torchmate 2x2 cnc table
    SMITHY 1324 mill/lathe
    60 gal. 7.5 hp air compressor


    MY YOUTUBE CHANNEL: https://www.youtube.com/user/dzljon/videos

Similar Threads

  1. Torchmate AVHC with PP60s
    By FeddFab in forum Everlast Plasma Cutters (PAC)
    Replies: 2
    Last Post: 01-04-2015, 06:27 PM
  2. Plasma & Torchmate
    By worntorn in forum Everlast Plasma Cutters (PAC)
    Replies: 23
    Last Post: 07-05-2011, 02:52 AM
  3. Power Plasma 50 & Torchmate 2 x2
    By geezer in forum Everlast Plasma Cutters (PAC)
    Replies: 11
    Last Post: 08-08-2010, 04:47 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •