Originally Posted by
broberts5
About 3months. It's sad. I know my machine wasn't abused or struck by lightening. I have put in calls to Ray, written 2emails to Oleg, no response!
Very concerning to hear that. I've been interested in buying an Everlast machine and was just beginning to look again. From what I read it seems they are really good welding machines at an unbeatable values when everything works right.. but the long repair time, how common issues appear to be + having to pay freight both ways is quite concerning. Perhaps we only hear about the bad on the forum and not all of the ones that work fine for the long haul, but it's concerning nonetheless.
New to welding!
Lots of Snap-On tools
In need of more toys