Share
Results 1 to 6 of 6

Thread: Powerpro 164 will 6011 work?

  1. #1
    Join Date
    Sep 2014
    Location
    Arley, Alabama, United States
    Posts
    6

    Default Powerpro 164 will 6011 work?

    I found out the hard way 6010 doesnt work worth a .... with this machine.
    Can I run 6011?
    If so what will work best DCEP or AC?

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by JCheney View Post
    I found out the hard way 6010 doesnt work worth a .... with this machine.
    Can I run 6011?
    If so what will work best DCEP or AC?
    DCEP usually works best. Some brands/machine combinations favor one or the other.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    No it won't weld 6010 and have never claimed it would. 6011 should be doable without any issue with DCEP.

  4. #4
    Join Date
    Sep 2014
    Location
    Arley, Alabama, United States
    Posts
    6

    Default

    Before I decided to buy it I didn't think to look through the forum to find out if it would run 6010. Just kinda figured it would..... oopps....

    I'll give 6011 DCEP a shot tomorrow. Definitely cant turn out as bad as the 6010 "beads" did. LOL. It was embarrassing to look'em even with no one around

  5. #5

    Default

    I found Lincoln Fleetwelds to work the best for me on most all the Everlast Equipment I've welded with. I haven't personally welded with the 164, but given what I know, I'd say that's a safe bet or Messer (US forge).

  6. #6
    Join Date
    Sep 2014
    Location
    Arley, Alabama, United States
    Posts
    6

    Default

    I forgot to update you guys.
    I'm running 3/32 sticks on 14 gauge mild steel
    I tried using prostar 6011 on DCEP........ ummm no
    prostar 6011 AC...... slightly better but still not consistent.
    (prostar 7014 runs decent by the way)
    Radnor 6011 DCEP runs better than the prostar stuff but your arc has to be REALLY short & you have to keep moving. Still have starts & stops on occasion but it works.
    Going to order fleetweld 6011
    Excalibur 7018MR runs beautifully
    I live way out in the sticks and lincoln electrodes aren't the easiest to come by otherwise I would have tried fleetweld 6011. Going to have to get some shipped to me.
    Thanks for the input guys!

Similar Threads

  1. 210 ext and 6011
    By girvin in forum General Welder Questions
    Replies: 5
    Last Post: 05-02-2015, 05:28 PM
  2. Powerpro 205s HF start does not work
    By 2005sxt24 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 12-31-2014, 01:32 PM
  3. 6011 or 7018?
    By travis in forum Stick Welding (SMAW)
    Replies: 28
    Last Post: 01-11-2014, 11:54 AM
  4. Harsh arc with 6011
    By posixPilot in forum Stick Welding (SMAW)
    Replies: 18
    Last Post: 04-04-2012, 11:53 PM
  5. PowerPro 256 6010/6011
    By DannyB1954 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 03-27-2012, 03:15 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •