    Hi all. I recently bought a 2Lb roll of the HF Flux Core. 0.030". Had a coupon for $15. Saw it was made in Italy. So I figured give it a try. Haven't opened it yet. Thinking about returning it. And sticking with the Hobart brand. However the Hobart is $5-$10 More roll. Has anyone used the HF Flux Core? And what is their opinion? Vs the Hobart or Lincoln brands?

    Thanks

  2. #2
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default

    We don't have HF up here but our nearest equivalent also carried an Italian flux core, so probably it's the same. I think it was INE brand ER something ending in GS? It was much worse than the Lincoln stuff: the arc wasn't as well defined and it produced a lot more spatter.
    If you're new to welding and need to get some seat time, it's fine. In fact you probably won't even notice the difference at that stage. At the time I swore off of it (burned about 3 or 4 rolls) money was pretty tight, but even so I abandoned a couple rolls I had. Ten years later they're still sitting there unused.
    I haven't tried Hobart so I can't comment on that.

  3. #3
    Join Date
    Aug 2014
    Location
    Trenton, New Jersey, United States
    Posts
    263

    Default

    Thanks. It was "E71T-GS", 2 Lb. Roll. Same thing I thought. Just Returned it. I may just stick to the Hobart brand when I need FC.

  4. #4
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default

    Quote Originally Posted by Elantramax1 View Post
    Thanks. It was "E71T-GS", 2 Lb. Roll. Same thing I thought. Just Returned it. I may just stick to the Hobart brand when I need FC.
    Yeah, that's the same stuff.

    Out here no-one I've found does anything other than rental bottles, so if you're only into occasional welding you get stuck with FC. The bottle costs more than the car you're fixing the rust holes on.

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Elantramax1 View Post
    Hi all. I recently bought a 2Lb roll of the HF Flux Core. 0.030". Had a coupon for $15. Saw it was made in Italy. So I figured give it a try. Haven't opened it yet. Thinking about returning it. And sticking with the Hobart brand. However the Hobart is $5-$10 More roll. Has anyone used the HF Flux Core? And what is their opinion? Vs the Hobart or Lincoln brands?
    If I find myself shopping for flux core, I usually just scrounge up a big piece of cardboard and some gaffers tape, instead.
    Long arc, short arc, heliarc and in-the-dark!

  6. #6

    Default

    Quote Originally Posted by Rambozo View Post
    If I find myself shopping for flux core, I usually just scrounge up a big piece of cardboard and some gaffers tape, instead.
    Or drill and safety wire
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. #7
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by everlastsupport View Post
    Or drill and safety wire
    There is that, but I was thinking of a wind break so I could use solid wire MIG instead of FC. Or just go to stick welding and be done with it.
    Long arc, short arc, heliarc and in-the-dark!

  8. #8

    Default

    Quote Originally Posted by Rambozo View Post
    There is that, but I was thinking of a wind break so I could use solid wire MIG instead of FC. Or just go to stick welding and be done with it.
    hahaha.. Sorry, thought you were making a joke. We have used big sheets of cardboard many times, and no fires, surprised. Stick or MIG would solve the wind.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Flux Core?
    By Elantramax1 in forum General Welding Questions
    Replies: 57
    Last Post: 09-29-2014, 12:25 PM
  2. Welding with flux core wire
    By Chris A in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 6
    Last Post: 06-08-2014, 05:20 AM
  3. Imig200 flux core welding questions
    By sw2x in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 17
    Last Post: 03-30-2013, 10:24 AM
  4. IMIG-200 with flux core, running on generator
    By chadford in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 6
    Last Post: 10-08-2011, 10:04 PM
  5. Gas vs flux core
    By MigPlazArc in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 17
    Last Post: 10-06-2011, 03:11 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •