Share
Results 1 to 9 of 9

Thread: PowerTIG 200DX Dual Voltage Gas Inlet Fitting Size

  1. #1

    Default PowerTIG 200DX Dual Voltage Gas Inlet Fitting Size

    What size is the gas inlet fitting size on the PowerTIG 200DX Dual Voltage? I have already tried a 1/4 in barbed fitting for my Victor 2400 Flowmeter from my local weld shop but it was too small for the fiber reinforced hose supplied with the welder. Please advise. Thanks.
    Everlast 200DX Dual Voltage
    ThermalArc 181i
    Lincoln ProCut 25
    Victor O/A Torch
    Jackson Pro Variable
    Jackson HSL100 Passive w/Phillips Gold #10
    Tweco Weldskill Auto-Darkening

  2. #2

    Default

    Do you have one with a hosebarb? or threaded fitting. If it's threaded then it's 5/8" CGA. If not, I think it's 5/16 hose barb. Usually 1/4" can be fit onto 5/16" hosebarb if there is any flex at all in the line. We've been using 5/8" CGA for a while now on most of our units.

  3. #3

    Default

    Thanks, Performance.

    I picked up another 5/16 barbed fitting to splice to a WA Technology Gas Saver System.

    5/8 in. CGA would be much easier for us in the U.S. If the new units come with that fitting that would be considered a move forward.
    Everlast 200DX Dual Voltage
    ThermalArc 181i
    Lincoln ProCut 25
    Victor O/A Torch
    Jackson Pro Variable
    Jackson HSL100 Passive w/Phillips Gold #10
    Tweco Weldskill Auto-Darkening

  4. #4

    Default

    No, we don't have any plans for the 5/8". That's a move backwards. I suspect you'll start seeing other brands with a quick connect like this. Lincoln already uses them on some of their product. The 5/8" is slow and aggravating to connect up compared to it. Europe uses them as well. There are plenty of sources of the quick connects as they have become standard. We sell them, Arc Zone sells them, and many others.

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    I think he was talking about the gas inlet, which you said you are making "B" CGA, but he has a hose barb version.
    Long arc, short arc, heliarc and in-the-dark!

  6. #6

    Default

    It's a 5/8" CGA. Not sure how old his unit is.

  7. #7

    Default

    Yes, I was talking about the gas inlet which on my machine is a barbed fitting. I purchased the PowerTIG 200DX Dual Voltage Welder October of 2013.
    Last edited by MBfrontier; 09-24-2014 at 07:25 AM.
    Everlast 200DX Dual Voltage
    ThermalArc 181i
    Lincoln ProCut 25
    Victor O/A Torch
    Jackson Pro Variable
    Jackson HSL100 Passive w/Phillips Gold #10
    Tweco Weldskill Auto-Darkening

  8. #8

    Default

    Not sure, but you may have gotten one of the last ones to have it of that model.

  9. #9

    Default

    Here it is:
    Click image for larger version. 

Name:	IMG_0897.jpg 
Views:	574 
Size:	132.3 KB 
ID:	12386
    Everlast 200DX Dual Voltage
    ThermalArc 181i
    Lincoln ProCut 25
    Victor O/A Torch
    Jackson Pro Variable
    Jackson HSL100 Passive w/Phillips Gold #10
    Tweco Weldskill Auto-Darkening

Similar Threads

  1. HF Start Points Adjustment on Powertig 200DX Dual Voltage
    By MBfrontier in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 02-25-2014, 02:03 PM
  2. PowerTig 185 Micro Dual Voltage
    By nils in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 10-24-2013, 11:04 AM
  3. 2013 Powertig 200DX 200 Amp 110/220 Dual Voltage Pulse AC/DC
    By magichat in forum TIG Welding (GTAW/GTAW-P)
    Replies: 21
    Last Post: 09-23-2013, 05:22 PM
  4. NEW 2013 Everlast PowerTIG 200DX AC/DC TIG DUAL VOLTAGE welder
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 28
    Last Post: 03-04-2013, 02:23 AM
  5. PowerTIG 185 Micro Dual Voltage??
    By Gtig in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 02-11-2012, 02:52 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •