Quote Originally Posted by Elantramax1 View Post
The replacement blade finally arrived. New 66T for Thick Gauge. When my finances improve, I need to get one for Lighter gauge.

Also the Northern Tools adapter arrived. Haven't had a chance to open it. Too busy working on the plate for the rear wheels. Smoothed it down a little more. Drilled the mounting holes for the casters. Clamped in place. Tomorrow I am doing the plug Welds. Still need to attach the bottom shelf. Not sure if I have enough Gas to do that. I may just drill the holes. And some of the Plug Welds to hold it. Until I can get the tank refilled. On a side note, Just checked the 2 pound roll of .030. Maybe 1/2 Pound left. Should be enough. I have an extra roll just in case.
Good news on the blade. Sounds like you got a good deal. Sometimes good deal takes a little work .

Yea, the gas will go a little faster on the first few tanks, but you will see over time your setting will get better and arc length will allow less gas too.

Maybe keep Flex core around just in case, we have two large CO2 and Stargon tanks, but I would do that in your case. Or keep some 6011/6013 around for a pinch.

Down here you can't get gas on the weekends. We can get steel at A1, but pay the price.