    Hello all. I purchased this PowerUltra 250P back in october 2011. It has been working very well if i say so myself TIG welding 304/316 stainless and very occasional plasma.

    The problem I have now started as a quiet fast ticking on the fan end of the unit every time I turned the welder on. This ticking went on for about a day or two then, as I was using it yesterday, the ticking went from quiet to much much louder. It was obvious there was something wrong so I looked in the fan end of the unit and nothing was obviously wrong. But upon very close inspection, I see a hairline cracks which have formed on the center plastic of the fan (not the fan blades but where the blades attach) starting from the outside and going into the middle where the bearings are.

    So what is happening is that when the fan starts, the centrifugal forces that are being placed on the fan are making the cracks want to separate and this then causes the fan to grind on the inside diameter of the fan shroud. It sounds like it will tear itself apart soon.

    Has anyone els ever had this happen to the fan in their unit?

    All in all, I like the unit although at this point I cannot use it until the fan gets replaced

    Also, the unit is within it's 5 year warranty. What do I need to do to get this taken care of?

    Thank-you for any helpful replies
    Last edited by Orlando; 09-12-2014 at 06:30 PM.

  2. #2

    Default

    Contact technical support. ext 207. Warranty process is listed on our website.

  3. Default

    Quote Originally Posted by performance View Post
    Contact technical support. ext 207. Warranty process is listed on our website.
    I contacted technical support as you mentioned and spoke to Ray. I explained the problem and he had me call another extension where they say they will be sending me a new fan but I have to pay shipping which is fine. Warranty on this problem was painless and to the point. I'm a happy camper. I'll update here when the part arrives and I install it. Maybe I'll post a pic of what I am welding with this machine once it gets up and running again. Hoping all goes as planned.

    Thanks EVERLAST!!

Similar Threads

  1. Power Ultra 250P Tig problem
    By kencal51 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 11-13-2015, 10:15 PM
  2. Power I-MIG 250p
    By Yofish in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 0
    Last Post: 02-25-2015, 05:25 AM
  3. Power I-IMIG 250P questions
    By Diabolical in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 11
    Last Post: 02-13-2012, 10:05 PM
  4. Questions about the TIG Pulse Option on the Power Ultra 250p
    By Haku in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 13
    Last Post: 06-08-2011, 04:54 PM
  5. Received my Ultra 205 Combo Unit Friday!
    By BigMacWelds in forum Customer Testimonials
    Replies: 0
    Last Post: 06-08-2009, 10:55 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •