Hi all. I am trying to weld 16 gauge square tube to a 1/4" plate. And seem to have trouble getting a good looking bead. I am using .030 Hobart FC. And an I Mig 140E. I am having trouble finding the correct V and Wire feed. Comes out clumpy.
Thanks
Elantramax1