No, you'd increase it by injecting air into the weld stream and increase oxidation. And likely destabilize the arc with the flow. Get some nozzle dip or spray if it is a problem...or trim the nozzle back if you aren't using it with gas.
No, you'd increase it by injecting air into the weld stream and increase oxidation. And likely destabilize the arc with the flow. Get some nozzle dip or spray if it is a problem...or trim the nozzle back if you aren't using it with gas.
Mark