    Hi all. I am new to this forum. And a proud owner of a Power I mig 140E. I am using Flux Core. And was wondering Why, Cant I use low pressure air on the gas port?? To keep the Nozzle clean. And possibly reduce some of the smoke and dust.

    I have the Clamp on the Positive. ground to the Torch. Using Hobart .030 FC. And am trying to get a better weld.

    Thanks
    Elantramax1

  2. #2
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Welcome to the forum, and congrats on the new machine!

    Are you thinking of supplying compressed air through the gun during the FCAW welding process?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  3. #3
    Join Date
    Aug 2014
    Location
    Trenton, New Jersey, United States
    Posts
    263

    Default

    I was wondering if it(Low PSI Maybe 5) would keep the Nozzle clean. And maybe reduce the dust and smoke from the welding.

  4. #4

    Default

    No, you'd increase it by injecting air into the weld stream and increase oxidation. And likely destabilize the arc with the flow. Get some nozzle dip or spray if it is a problem...or trim the nozzle back if you aren't using it with gas.

  5. #5
    Join Date
    Aug 2014
    Location
    Trenton, New Jersey, United States
    Posts
    263

    Default

    Thanks Mark. I was able to find a small brush made by Forney that will be able to clean the inside of the Nozzle. Its made of Nylon I think. Definitely not metal. Could I use low PSI air to blow out the diffuser from time to time? Run it through the gas port. But not actually welding.

    Thanks
    Elantramax1

  6. #6

    Default

    Quote Originally Posted by Elantramax1 View Post
    Thanks Mark. I was able to find a small brush made by Forney that will be able to clean the inside of the Nozzle. Its made of Nylon I think. Definitely not metal. Could I use low PSI air to blow out the diffuser from time to time? Run it through the gas port. But not actually welding.

    Thanks
    Elantramax1
    You can take the nozzle off for flux core. There are even flux core nozzles for tweco guns that taper down to the contact tip with no opening.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. #7
    Join Date
    Aug 2014
    Location
    Trenton, New Jersey, United States
    Posts
    263

    Default

    zoama, I Tried a couple of different Nozzles. Hobart, Lincoln. Wont fit. The I Mig 140E uses a Binzel torch with Tweco Series 11 contact tips. The Lincoln/Tweco tips fit. Not the Nozzles. I even tried an Eastwood Spot Weld nozzle. Had to return that as well.

    I leave the Nozzle on to protect the Spring and Diffuser.

    I am running Hobart .030 F-Core. 2 pound roll on sale for $15. Good thing I snagged one. Price went up.

  8. #8

    Default

    Quote Originally Posted by Elantramax1 View Post
    zoama, I Tried a couple of different Nozzles. Hobart, Lincoln. Wont fit. The I Mig 140E uses a Binzel torch with Tweco Series 11 contact tips. The Lincoln/Tweco tips fit. Not the Nozzles. I even tried an Eastwood Spot Weld nozzle. Had to return that as well.

    I leave the Nozzle on to protect the Spring and Diffuser.

    I am running Hobart .030 F-Core. 2 pound roll on sale for $15. Good thing I snagged one. Price went up.
    Run an .035 tip with that stuff for less hangups. Did you swap polarity to electrode negative for flux core ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  9. #9
    Join Date
    Aug 2014
    Location
    Trenton, New Jersey, United States
    Posts
    263

    Default

    Torch to Neg, Clamp to Pos

Similar Threads

  1. Stupid newbie question
    By breakneckmot in forum General Welding Questions
    Replies: 9
    Last Post: 09-17-2013, 06:58 PM
  2. Some stupid questions
    By dennis in forum Pre-sales, Sales and Shipping questions
    Replies: 2
    Last Post: 12-08-2011, 10:03 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •