Share
Results 1 to 9 of 9

Thread: HF starts quit working - PowerTIG 200DX

  1. #1

    Question HF starts quit working - PowerTIG 200DX

    Has anyone else had issues with HF startups failing? Had DX200 new since Feb 2014, and it's only seen enough operation to see one #3 bottle argon replacement. Just recently the HF stopped completely as if the switch was stuck on lift-start. In other words, even the switch set in the HF position; I had to do lift/scratch starts on my mild steel project (DC). ? I've checked & re-checked grounds, torch, pre-flow settings, and of course the Lift/HF/stick 3-posistion switch. With the exception of no HF starting, the welder welds fine.

    So I called Everlast support, and the call was helpful. We reviewed correct settings, even toggled every switch and knob just for the sake of it, including reconnecting all cables at the front - yet still no HF. Again, unit welding fine - just no more HF starting.

    Update:
    Two days later, purely on curiosity, I decided to see how bad this no HF thing is going to affect future AC (aluminum) jobs. Low and behold HF working fine now !! So I went back to DC and HF working there too. Odd ... can't explain why HF is working again. I sure hope this is not an intermittent problem now. Thought I'd pose the question in case there’s some "gotchya" setting I missed.

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Did you ever check the point gap?
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    Point gap? Nope. Not farmiliar with troubleshooting welders, but I was just about to pop the cover when hf started working again.
    That said, I'm inclinded to do nothing until it fails again.
    Is the point gap something inside?

  4. #4

    Default

    Quote Originally Posted by Timebandit View Post
    Point gap? Nope. Not farmiliar with troubleshooting welders, but I was just about to pop the cover when hf started working again.
    That said, I'm inclinded to do nothing until it fails again.
    Is the point gap something inside?
    It is inside and should be set to .030" Sounds like they are a little out.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. #5

    Default

    I had problems with my hf when i first got my 250 ex and had to reset them when i called everlast and it worked great after that.
    250 ex
    205 mig
    milwaukee grinder
    140e mig

  6. Default

    My 200DX (2/2014) will not HF start while DC welding once in a while. Sometimes I just try to initiate an arc again and it works, sometimes I have to move the ground clamp and it works. I figured it was due to something I was doing. I have not found it to be too much of an annoyance...yet, it only does it maybe once every 50 HF starts. I hope it is not something that will begin to occur more often, then again the 5yr warranty makes my worries go away.

  7. #7
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Beginner View Post
    My 200DX (2/2014) will not HF start while DC welding once in a while. Sometimes I just try to initiate an arc again and it works, sometimes I have to move the ground clamp and it works. I figured it was due to something I was doing. I have not found it to be too much of an annoyance...yet, it only does it maybe once every 50 HF starts. I hope it is not something that will begin to occur more often, then again the 5yr warranty makes my worries go away.
    Check the points. A simple adjustment could save you a lot of headaches down the road.
    Long arc, short arc, heliarc and in-the-dark!

  8. #8

    Default

    Check the points. Make sure there are .030 or .025 range. Should solve the problem. Make sure the machine is unplugged, and remove the cover from the back panel, not the front.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  9. #9

    Default

    Also,
    HF starting percent is not 100%. It is close, but the name brands such as Miller have had machines that would only start well less than that percent such as the units before this current generation of Dynasty. It should be close though to the 100% mark. But there are factors that can interfere with starting percentages too, as you seem to know. Small issues, such as not connecting the clamp directly to the work and oxidation at the work clamp or possibly a loose connector or cable can all create transient problems that are hard to pinpoint.

Similar Threads

  1. 185 solenoid quit working..??????
    By stretch in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 06-30-2016, 05:49 AM
  2. Foot pedal does not stop arc sometime, now my 200DX is not working
    By ostie01 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 06-07-2014, 03:27 PM
  3. 2010 200DX HF start not working
    By mbppg in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 02-04-2014, 12:10 PM
  4. PowerTig 250ex not working...
    By chris.hindley in forum TIG Welding (GTAW/GTAW-P)
    Replies: 13
    Last Post: 03-30-2011, 01:48 PM
  5. PM 256 Hi-Freq quit working
    By Tony_F in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 8
    Last Post: 08-19-2010, 09:12 PM