Im welding with 6061 t6 Aluminum .090 and some how my machine was reset and I lost my settings. since that happen I can't seem to get my welder to perform as good as it was. Can anyone give me there settings so I can readjust my machine? Below are my settings
2% lanthinated
100 amps
25 argon
1 pre flow
7 post flow
30 pulse amps
1 hot time
50% arc force
50 frequency
-15 cleaning balance
advanced square
0 up slope
0 down slope