    To be clear even a piece of alum. that had the oxide coating cleaned off of it one day should be cleaned again if the welding on it is not completed within the same day . I personally would not clean it again unless it was a critical part that needs top strength, like an airplane part .
    Miller 302 gas drive
    millermatic 200 mig
    miller spoolmatic 3 spool gun with 100ft ext.
    2014 Everlast PP60S plasma
    thermal arc 250 GTS inverter
    2016 Everlast 250EX
    miller tig cooler
    2015 Everlast MTS250S
    Miller 30A spool Gun
    Miller xtreme 12VS wire feeder
    Linde CM 85 shape cutter

Similar Threads

  1. aluminum welding with mig
    By rebelbah in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 2
    Last Post: 10-18-2016, 04:36 PM
  2. mig welding aluminum
    By Rodsmachineshop in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 3
    Last Post: 06-20-2012, 11:50 AM
  3. tig welding aluminum with a DC only tig
    By rab in forum General Welder Questions
    Replies: 18
    Last Post: 04-03-2012, 02:25 AM
  4. Replies: 2
    Last Post: 08-03-2011, 03:50 PM
  5. Tig welding aluminum
    By Tallguy64 in forum General Welding Questions
    Replies: 6
    Last Post: 04-10-2010, 11:02 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •