  1. Default Welding on compressor air tank

    My small 45 year old 3/4 hp compressor air tank needs to be replaced.

    Is it ok to weld the air pump and motor base onto a new tank?

    The factories obviously do it; just not sure if there are any safety issues, and how they are dealt with.

    Thanks,
    rivets

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Rivets View Post
    My small 45 year old 3/4 hp compressor air tank needs to be replaced.

    Is it ok to weld the air pump and motor base onto a new tank?

    The factories obviously do it; just not sure if there are any safety issues, and how they are dealt with.

    Thanks,
    rivets
    Welding pressure vessels is not something you want to experiment with. You have to know what you are doing and go through plenty of destructive and non-destructive testing to become certified it that field. The tuition for the school of hard knocks for that can literally be an arm and a leg or much worse.

    Build your pump and motor mount then attach to the tank with some steel bands, instead. Or buy a tank with mountings on it. Tanks are hydro tested after they are all welded up. So even if you have the skill, it's not worth it to do the testing.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    Quote Originally Posted by Rambozo View Post
    Welding pressure vessels is not something you want to experiment with. You have to know what you are doing and go through plenty of destructive and non-destructive testing to become certified it that field. The tuition for the school of hard knocks for that can literally be an arm and a leg or much worse.

    Build your pump and motor mount then attach to the tank with some steel bands, instead. Or buy a tank with mountings on it. Tanks are hydro tested after they are all welded up. So even if you have the skill, it's not worth it to do the testing.
    Beyond Ditto... My brother "knew" a guy that had a truck split rim take his head off. The air will expand inside if you heat it.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. Default

    Thanks, Rambozo and Mike.

    rivets

Similar Threads

  1. Tig welding a motorcycle gas tank
    By rake in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 04-09-2013, 03:42 AM
  2. Compressor???
    By Rafael in forum Everlast Plasma Cutters (PAC)
    Replies: 25
    Last Post: 02-12-2013, 03:32 AM
  3. Welding Tank Cart
    By Kempy in forum Other Custom Fabrications
    Replies: 13
    Last Post: 02-10-2013, 01:23 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •