Share
Results 1 to 7 of 7

Thread: Question on possible tungsten dip contamination.

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Question on possible tungsten dip contamination.

    Hello

    I've been practicing on tungsten gap and rod filler hand control, I touched the tungsten into the puddle a few times and noticed that the arc turned in to a bluish:green color I continued to weld and noticed some splatter and when I was done I also noticed a reddish/orange rust color around the areas of where the tungsten tuched the puddle. Now am I able to reuse the tungsten or would it be best to break of the effected piece of it ? Or regarding the end ? Also when I Reuse a filler rod is it recommended to clip the end from the pervious weld or will it be fine to add to the new puddle ?
    Thanks in advance
    Frank
    Powertig 200DX
    Lincoln 140 mig
    and a whole bunch of tools

  2. #2
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    If you dip the tungsten, best practice is to swap it out for another right away. You can re-sharpen the dipped one, rather than break it off. There's a lot of discussion about how to sharpen tungstens, so if you need a primer, just let us know.

    OK to re-use filler from puddle to puddle, no worries, because ideally you keep the filler rod within the envelope of shielding gas. Jody at WT&T has a video devoted to three TIG pitfalls to avoid, and keeping the filler inside the shielding gas envelope is one of them.

    Sounds like you're getting after it, good on ya!
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  3. #3

    Default

    Don't try to break lanthanated tungsten... it will splinter lengthwise.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4

    Default

    Thanks , what is a primer ?
    I'm using the harbor freight diamond wheel that was recommended by welding tips and tricks,
    On a drill , making sure to grind it inline with tungsten.
    Last edited by Frank; 06-25-2014 at 01:15 AM.
    Powertig 200DX
    Lincoln 140 mig
    and a whole bunch of tools

  5. #5

    Default

    Quote Originally Posted by Frank View Post
    Thanks , what is a primer ?
    Help getting started... like priming a pump.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. #6

    Default

    Quote Originally Posted by zoama View Post
    Help getting started... like priming a pump.
    Ahhhh yeah makes sense now, lol ... Nice one
    Thanks for the information guys , very helpful !
    Powertig 200DX
    Lincoln 140 mig
    and a whole bunch of tools

  7. #7
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Quote Originally Posted by Frank View Post
    I'm using the harbor freight diamond wheel that was recommended by welding tips and tricks,
    On a drill , making sure to grind it inline with tungsten.
    Sounds like you've got it covered... you can skip to the back of the book!
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

Similar Threads

  1. Tungsten dressing question
    By Winky in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 06-07-2012, 02:18 AM
  2. Perhaps a silly question about tungsten...
    By Trip59 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 05-28-2012, 11:25 PM
  3. Tungsten size question.
    By Brian Ski in forum TIG Welding (GTAW/GTAW-P)
    Replies: 22
    Last Post: 03-25-2012, 08:06 PM
  4. Tungsten Question
    By SeanMurphy265 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 09-12-2011, 04:22 AM
  5. Tungsten grinder question
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 09-06-2011, 06:53 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •