If your burning up your cups, then you are doing something wrong, or there is another problem. I have used those torches for months, really, almost a year without burning them up. That torch is not designed for a ceramic cup and it is completely different in design. The plastic is a heat resistant plastic, more like bakelite. Excessive piercing, cutting in blind holes, wrong start angle allowing too much blow back(straight down in thick metal will do it), cutting at or near maximum cut for extended periods of time at maximum amps, or any condition that causes too much blowback will speed up destruction of the cup.

But no, there will never be a ceramic cup offered for the torch on that model, unless the torches change.