    Default modified harbor freight cart

    I made an extension panel to fit the machines and bent tubing for handles, bought the carts for $35 each
    Click image for larger version. 

Name:	photo 3-3.jpg 
Views:	1446 
Size:	118.1 KB 
ID:	12136Click image for larger version. 

Name:	photo 4-2.jpg 
Views:	1399 
Size:	143.5 KB 
ID:	12137Click image for larger version. 

Name:	photo 1-4.jpg 
Views:	1288 
Size:	136.5 KB 
ID:	12138Click image for larger version. 

Name:	photo 2-4.jpg 
Views:	1266 
Size:	121.7 KB 
ID:	12139
    Last edited by dzljon; 06-13-2014 at 01:01 AM.

Similar Threads

  1. Harbor Freight Welding Cart
    By Depdog in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 15
    Last Post: 02-05-2018, 06:30 PM
  2. $39 Harbor Freight tungsten sharpener
    By DaveBonds in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 14
    Last Post: 03-22-2014, 01:35 PM
  3. modified my cart
    By single t gt in forum Other Custom Fabrications
    Replies: 0
    Last Post: 04-17-2011, 11:36 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •