    Default Argon / co2 question

    Another thread touched on this, but I didn't want to hijack that thread.

    In MIG argon /co2 high pressure cylinders of shielding gas, does the co2 component exist in its gaseous or liquid state?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  2. Default

    Straight CO2 stays a liquid under moderate pressure

  3. #3
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Quote Originally Posted by res0r9lm View Post
    Straight CO2 stays a liquid under moderate pressure
    100% Co2 at 68 F pressure is around 840 PSIG in liquid state in a high pressure cylinder, as you use the Co2 gas its pressure will not change in the tank until you used up all the liquid. The gas at the top of the liquid will stay at 840 PSIG as long as the temperature dose not change. Once the pressure drops below 840 PSIG at 68 deg. F or 20 deg. C it will keep going down till it is empty.
    Once you mix Co2 with Argon they are both in a gases state. Now put 25% Co2 mix with Argon by pressure it should be 250 PSIG Co2 to 750 PSIG Argon at 68 deg. F but that is OK if you only need 1000 PSIG of C25/A75 mix. So in a 2400 PSI tank they put in 675 PSIG of Co2 in the tank and fill it to 2400 psig with Argon at 68 Deg. F with a temperature controlled blending machine this is what I was told by the welding supplier I get my gas from.
    Next time I go into the mixing plant part I will ask if I can take any pictures.
    Last edited by Kempy; 06-08-2014 at 03:56 PM.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  4. #4
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Thanks, Kempy, I'd be interested to see pictures.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by DaveO View Post
    Another thread touched on this, but I didn't want to hijack that thread.

    In MIG argon /co2 high pressure cylinders of shielding gas, does the co2 component exist in its gaseous or liquid state?
    My initial take is that the two become a compound, and stay gaseous. This is just from the feel of the cylinder. You can feel liquid sloshing around in a CO2 cylinder, even if it's pretty low, yet you don't feel that in a C25 cylinder, even when full.

    Next time I pickup a C25 cylinder, I guess I can verify that by inverting it, and crack the valve open a little.
    Last edited by Rambozo; 06-08-2014 at 12:30 AM.
    Long arc, short arc, heliarc and in-the-dark!

  6. #6
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    I searched a couple other welding forums with no conclusive results, and searched a couple MSDS sheets for "LIQU" strings with no results. I may give Airgas a call to see if they have a definitive answer.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

Similar Threads

  1. 100 PSI argon flo?????
    By stretch in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 32
    Last Post: 06-09-2016, 09:51 PM
  2. Why 100% Argon or Argon/CO2 75/25%
    By mdennis in forum General Welding Questions
    Replies: 6
    Last Post: 08-09-2013, 05:11 AM
  3. Air/Argon
    By ChadP in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 11
    Last Post: 02-09-2013, 10:20 PM
  4. Just a question about Argon from the LWS.....?
    By CGCINC in forum TIG Welding (GTAW/GTAW-P)
    Replies: 15
    Last Post: 02-17-2012, 02:22 AM
  5. ARGON and ARGON/CO2 TANK SIZES
    By everlastsupport in forum Technical Bulletins and Tips
    Replies: 47
    Last Post: 10-13-2011, 06:19 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •