  1. Angry Foot pedal does not stop arc sometime, now my 200DX is not working

    Like the title says, when I release the foot pedal, sometime the arc will not stop completely, I mean the amp goes down but, still get an arc.

    Last night, I was welding and it happen again, Now there is a hissing sound inside the welder, tought it was

    a gas leak but, when I look inside the welder at the front, I can see an arc ( I think it called spark gap).

    Now, as soon as I turn on the welder, the arc is on, I turn it off after one or two seconds.

    I really need my welder to finish a job I was working on.

    My welder is only a couple months old, maybe 5 or 6 months and have maybe 25 hours of welding time with it.

    Is there anything I can do to fix it.

    Thanks for your time.

    On the welding forum, they prefer to argue about a ####ing 2T/4T function that does not exist instead of helping me trying to find a solution to my problem


    Jeff

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Sounds like the switch in the pedal is out of adjustment. You can find some posts here with photos of whats inside. It should not be that tough to make that adjustment. It is normal for the HF arc points inside to spark for a bit when you first turn on the machine as they do a self test. But if the pedal switch is stuck on they will go much longer. You can check this by unplugging the pedal then power up the machine.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    I am not sure, as I did not see the forum flag your post as new, as I look for the bold print. I have not seen it bold. But anyway,
    Rambozo is right on all accounts here, when see the spark that is the HF which is stuck on. I suggest you check the pedal switch too. This forum is where we provide tech support for the welders primarily and is where we tune in to see if there are any customer issues. WW is well, not that type of forum typically to say the least. If it won't work, after checking the torch switch and the foot pedal to eliminate all possibilities, I'd call tech support directly.

  4. Default

    Great to receive some feedback here.

    Will make some tests and update my thread.

    Thanks a lot.

    Jeff

  5. Default

    Ok, unpluged the connector for the foot pedal and everything looks OK, if I hoock up the connector, the arc start fire up again,

    so trouble is in the foot pedal.

    Thanks, Jeff

  6. Default

    Ok, problem solved, just bent the micro switch lever a bit and it work.

    Thanks, Jeff

Similar Threads

  1. 200dx pedal stopped working properly
    By deathguppie in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 04-06-2015, 04:28 PM
  2. Foot Pedal issue. PowerTig 200DX analog
    By Challenger in forum TIG Welding (GTAW/GTAW-P)
    Replies: 20
    Last Post: 09-14-2014, 01:32 AM
  3. 2010 200DX HF start not working
    By mbppg in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 02-04-2014, 12:10 PM
  4. PowerTig 225LX Foot Pedal stopped working, How to Ohm Test?
    By Welderooni in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 12-18-2012, 06:40 AM
  5. WTB: Foot Pedal for 200dx
    By budracer1 in forum Buy, Sale or Trade
    Replies: 3
    Last Post: 10-14-2012, 01:14 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •