I got this welder a little over a year ago but didn't have power set up for it until early this year. It welds somewhat ok, but it pulses a lot in the higher amp settings. I'm running 0.045 flux core wire. The power supply seems fine and I run a power plasma 80 on the same circuit just fine at 45 amps output. That thing is awesome. The length of wire stickout varies a lot, several times per second and it's really hard to get a good weld out of it. It's just as if someone is turning the wire feed speed up and down really fast while I'm welding. I've noticed the wire feed speed readout and the volt output numbers also vary in the same way during welding. Anyone have any thoughts? Any help is greatly appreciated.


 
					
					 
							