    Im having a problem of not having any amperage control using the foot pedal on tig. Its either idle or straight to the set amps when you move the pedal the slightest amount. Ac or dc, it dont matter. The pedal an ssc control with the 50k pot. Machine is set to 2t, start/end apms at minimum, up/down slope at minimum aswell. Whats sucks is i sent the machine in for warranty where they had it for 4 months and its still not fixed. Theyre claiming its a pedal but the pedal ohms out at pin 3-4 is .9-48.1k and pin 4-5 is 48.1-.9 ohms. So its well within the +/-10% they say is acceptable. Any suggestions on what to do. Any help is appreciated

  2. #2

    Default

    Yeah, it's probably not the pedal. But you can never be sure. Contact ext 201 in the morning and explain the issue, that unit does what it did before...

  3. Default

    Make absolutely sure the pedals connector, on the machine, is tight. Maybe "spread" the pins a tiny bit to know they're making good contact...

    I chased weird pedal problems on my PP256 and 1/2 the time (because I was removing it so often) it turned-out to be the fact I wasn't tightening the ring on the plug each time

  4. Default

    Found the problem with the help of Ray. The short circuit of pin 6-7 telling the machine it has a pedal plugged in had a broken solder joint on a brand new pedal. Now it works like I want it which is a relief. Now to put it through some paces lol. Thanks for the help. Mike

  5. #5

    Default

    Quote Originally Posted by performance View Post
    Yeah, it's probably not the pedal. But you can never be sure. Contact ext 201 in the morning and explain the issue, that unit does what it did before...
    I think this is Mike and its was bad connecter on SSC pedal
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

Similar Threads

  1. Powerpro 205 tig pedal problem
    By toxicturtle in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 05-20-2016, 01:59 PM
  2. Wireless pedal for PowerPro 256?
    By ScottRussell in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 12-01-2012, 05:38 PM
  3. Problem with foot pedal on LX 225
    By brianscott in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 06-23-2011, 05:44 PM
  4. foot pedal problem
    By johnson697 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 12-17-2010, 03:06 PM
  5. superultra 205 foot pedal problem
    By agrrob in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 10-31-2010, 11:42 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •